Edge chipping or breaking
Sandvik, Mitsubishi and Iscar all say: use a tougher grade; lower the feed; use a stronger edge: a honed or chamfered edge, a larger nose radius.
What you see
Small chips missing along the edge, or a corner breaking off, often well before it is worn.
Causes and what to change
Every fix here is from Sandvik, Mitsubishi and Iscar's troubleshooting guides, unless marked. Change one thing at a time.
A grade too hard or brittle for the cut
Use a tougher grade
Feed or depth of cut too heavy for the edge
Lower the feed
Iscar: at the start of the cut too.
Take a lighter cut
Only Mitsubishi
An unstable setup or an interrupted cut
Use a stronger edge: a honed or chamfered edge, a larger nose radius
Make the setup more rigid
Built-up edge tearing off and taking bits of the edge with it
The fix is on Built-up edge: Raise the cutting speed.
Chipping: who gives which fix
Chipping: which maker gives which fix
| Fix | Sandvik | Mitsubishi | Iscar |
|---|---|---|---|
| Use a tougher grade | ✓ | ✓ | ✓ |
| Lower the feed | ✓ | ✓ | ✓ |
| Use a stronger edge: a honed or chamfered edge, a larger nose radius | ✓ | ✓ | ✓ |
| Make the setup more rigid | ✓ | ✓ | ✓ |
| Take a lighter cut | – | ✓ | – |
Work it out
Often comes with
Sources
Sources4
- Sandvik Coromant — Troubleshooting in turning (archived Dec 4, 2024)
- Mitsubishi Materials — Trouble shooting for turning (archived Jul 10, 2026)
- Mitsubishi Materials — Causes of tool damage (types of cutting edge damage and solutions)
- ISCAR — ISO turn inserts wear troubleshooting
Written in our own words from each maker's troubleshooting guide.