Long, stringy chips

Sandvik and Mitsubishi both say: raise the feed; take a deeper cut; use a smaller nose radius.

What you see

Chips come off in long ribbons or bird’s nests that wrap the part, the tool or the chuck.

Causes and what to change

Every fix here is from Sandvik and Mitsubishi's troubleshooting guides, unless marked. Change one thing at a time.

  1. Feed too light for the chipbreaker

    • Raise the feed

      Into the chipbreaker’s range; the box or catalog gives it.

    • Pick a chipbreaker made for this feed and depth

      Chipbreakers by maker
  2. Depth of cut too shallow to reach the chipbreaker

    • Take a deeper cut

      The chip needs to reach the chipbreaker to curl.

  3. Nose radius large for the depth of cut

    • Use a smaller nose radius

  4. A small entering angle (big lead) thinning the chip

    • Use a holder closer to a 90° entering angle (less lead)

      A thicker chip breaks more easily.

Other changes the makers name

  • Turn the coolant on, or aim it at the chip

  • Lower the cutting speed

    Only Mitsubishi

Work it out

Often comes with

Sources

Sources3