Chipbreakers
Each chipbreaker as its own maker prints it: the ISO groups it is made for, the cutting area, and the feed and depth window where the maker gives one, checked against the maker’s catalog. Open one for every other maker’s chipbreaker for the same job.
I pick the breaker for the depth I’m actually taking. A roughing breaker on a light finish pass just makes stringy chips.
Quick numbers
Each maker’s breaker for a medium cut, from the insert pickerSteel, medium cutP, mediumEach maker’s breaker for the same group and cut, with its own feed window
Stainless, medium cutM, mediumEach maker’s breaker for the same group and cut, with its own feed window
Calculators
Fix a problem
- Long, stringy chipsChips come off in long ribbons or bird’s nests that wrap the part, the tool or the chuck.
- Chips too short, hard or hammeredTiny chips that fly, weld together or hammer the edge; the cut sounds harsh and inserts chip early.
- Rough, torn or hairy finishThe finish misses the print: torn, smeared or scratched, or a feed pattern too coarse to pass.
Charts
Not listed: Walter (it names ISO groups per geometry, not a cutting area), and geometries no other maker’s verified chipbreaker can be compared with. Need one for a cut? Use the insert picker.
Kennametal · 13 chipbreakers
| Chipbreaker | Insert | ISO | Cutting area |
|---|---|---|---|
| FS | negative | S | finishing |
| LF | negative | M, S | finishing |
| FP | negative | M | finishing |
| MS | negative | M, S | medium |
| UP | negative | M, S | medium |
| P | negative | P, M, S | medium |
| MP | negative | P, N | medium |
| RP | negative | P, M, K | roughing, heavy roughing |
| LF | positive | P, M, K, N, S | finishing |
| UF | positive | P, M, K | finishing |
| FP | positive | P, M, K, S | finishing |
| MP | positive | P, M, K, S | medium |
| HP | positive | K, N, S | finishing |
Mitsubishi · 30 chipbreakers
| Chipbreaker | Insert | ISO | Cutting area |
|---|---|---|---|
| FS | negative | S | finishing |
| FJ | negative | S | finishing |
| LM | negative | M | light cuts |
| LS | negative | S | light cuts |
| MJ | negative | S | light cuts |
| MM | negative | M | medium |
| MS | negative | S | medium |
| GM | negative | M | light cuts, medium |
| ES | negative | M | medium |
| RM | negative | M | roughing |
| RS | negative | S | roughing |
| GJ | negative | S | roughing |
| HL | negative | M | heavy roughing |
| SH | negative | P | light cuts |
| GH | negative | P, K | roughing |
| HZ | negative | P | heavy roughing |
| FP | negative | P | finishing |
| MP | negative | P | medium |
| RP | negative | P | roughing |
| MK | negative | K | medium |
| RK | negative | K | roughing |
| AZ | positive | N | finishing |
| FM | positive | M | finishing |
| FS | positive | S | finishing |
| FS-P | positive | S | finishing |
| FJ | positive | S | finishing |
| MJ | positive | S | finishing, light cuts |
| MM | positive | M | medium |
| MS | positive | S | medium |
| MV | positive | P, M | medium |
Sandvik · 5 chipbreakers
Seco · 8 chipbreakers
| Chipbreaker | Insert | ISO | Cutting area |
|---|---|---|---|
| MF1 | negative | M, S | finishing, light cuts |
| MF4 | negative | M | finishing, medium |
| MF5 | negative | P, M | finishing, light cuts, medium |
| M1 | negative | S | light cuts, medium |
| M5 | negative | P, M, K | medium, roughing, heavy roughing |
| MR3 | negative | M, S, H | medium, roughing |
| MR4 | negative | S | medium, roughing |
| RR6 | negative | P, M | roughing, heavy roughing |
Guides
Sources
Sources4
- Mitsubishi Materials — General Catalog C010A, turning inserts: chip breaker classification (pp. A046–A070) (archived Nov 15, 2026)
- Kennametal — Master Catalog 2018, Vol. 1 Turning Tools (inch), chip control geometries (pp. B30–B35) (archived Jun 4, 2023)
- Seco Tools — Turning catalogue 2026.2: carbide chipbreakers (pp. 111–114) (archived Nov 16, 2026)
- Sandvik Coromant — Turning Handbook C-1020-18: geometry and grade, first choice for T-Max P and CoroTurn 107 (p. 2) (archived Nov 16, 2026)