Lathe

HSS lathe tool grinding

Rake, relief and edge angles to grind a high-speed steel lathe tool for your material.

Which tool?

For a hand-ground high-speed steel tool bit.

Right-hand turning tool for machine steel

Angles to grind, and where each comes from
AngleGrind
Side relief10–12°One source: US Army TC 9-524, the military’s machinist training manual
Front (end) relief8°One source: US Army TC 9-524, the military’s machinist training manual
Side rake12–18°One source: US Army TC 9-524, the military’s machinist training manual
Back rake8–15°One source: US Army TC 9-524, the military’s machinist training manual
Side cutting edge angle0° to cut up to a square shoulder; up to 30°15°US Navy Machinery Repairman manual, general figure for turning tools
End cutting edge angle8–30° in use; a little more for finishing15°US Navy Machinery Repairman manual, general figure for turning tools
Wedge (keenness) angle60–68°Geometry: 90° less the side rake and side relief
Nose radius1/64–1/32" (0.4–0.8 mm)US Navy Machinery Repairman manual, general figure for turning tools

The tool, drawn from these angles

From above: the cutting edges, 15° each.
From the side: back rake on top, front relief below.
From the front: side rake on top, side relief below.

Where the table gives a range, the drawing uses its middle. Not to scale.

Grinding order

  1. Grind the left side: the side cutting edge at 15° to the bit's side, with 10–12° side relief under it.
  2. Grind the right side back far enough to clear the work.
  3. Grind the front: the end cutting edge at 15°, with 8° front relief under it.
  4. Round the nose to 1/64–1/32" radius where the two edges meet.
  5. Grind the top: 12–18° side rake falling away from the cutting edge, and 8–15° back rake.
  6. Hone the cutting edge with an oilstone.

Dip the bit in water often: if it gets too hot to hold, it's too hot. The order follows South Bend's How to Run a Lathe.

What next

What speed and feed for this lathe cut?Lathe SFM, feed and depth of cut for your material and insert, with the RPM.
How deep, and how many passes, for this thread?Thread depth, compound setting, infeed per pass and a G76 line for lathe threading.
What’s wrong with this cut?Stringy chips, chatter, a torn finish, built-up edge or chipped inserts: causes and what to change.
How the hSS lathe tool grinding works

For machine steel, grind a high-speed steel turning tool with 10–12° side relief, 8° front relief, 12–18° side rake and 8–15° back rake (US Army TC 9-524), and 15° side and end cutting-edge angles with a 1/64–1/32" nose (US Navy). Pick your tool and material for the rest.

More

Sources

The Army's table is the one per-material table we could read; Little Machine Shop's sheet reprints it. The drawings are ours.