Tooling & workholding · Lathe tools
Lathe tool angles
A hand-ground high-speed steel tool for machine steel takes 10–12° side relief, 8° front relief, 12–18° side rake and 8–15° back rake, per the US Army’s TC 9-524. Aluminum takes the most rake: 15° side and 35° back; brass and bronze almost none: 5° to −4° side and 0° back, so the tool doesn’t grab. The chart gives all 8 materials.
HSS tool angles by material
Degrees. One source: US Army TC 9-524, the military’s machinist training manual, Table 7-1.
| Material | Side relief | Front relief | Side rake | Back rake |
|---|---|---|---|---|
| Aluminumwedge 63° | 12° | 8° | 15° | 35° |
| Brasswedge 75–84° | 10° | 8° | 5° to −4° | 0° |
| Bronzewedge 75–84° | 10° | 8° | 5° to −4° | 0° |
| Cast ironwedge 68° | 10° | 8° | 12° | 5° |
| Copperwedge 58° | 12° | 10° | 20° | 16° |
| Machine steelwedge 60–68° | 10–12° | 8° | 12–18° | 8–15° |
| Tool steelwedge 68° | 10° | 8° | 12° | 8° |
| Stainless steelwedge 60–65° | 10° | 8° | 15–20° | 8° |
Wedge (keenness) angle is 90° less the side rake and side relief. South Bend gives about 60° for mild steel and 80–85° for cast iron and hard steel. Each material opens the grinding wizard with its angles drawn.
The rest of the tool
- Side cutting edge angle: 15° for most rough turning; 0° to cut up to a square shoulder, up to 30° (US Navy).
- End cutting edge angle: 8–30°, about 15° for rough turning, a little more for finishing (US Navy).
- Nose radius: 1/64–1/32" for turning; too large chatters (US Navy).
- Parting and threading tools: no side rake, edge exactly on centre (South Bend). A thread tool is a 60° point, flat on top.
Sources
- US Army TC 9-524, Fundamentals of Machine Tools, Table 7-1: tool bit angles by material
- US Navy, Machinery Repairman 3 & 2 (NAVEDTRA, 1990), chapter 6: cutting tool angles
- South Bend Lathe Works, How to Run a Lathe (1934): grinding lathe tool cutter bits
Little Machine Shop's Grinding Tool Bits sheet prints the same numbers as the Army table, so it is the same source, not a second one.