Learn · 7 min
Grinding a HSS lathe tool
Relief under the edge keeps a lathe tool from rubbing and rake on top makes it cut; together they set the wedge angle, 90° less side rake and relief.
Relief keeps the tool from rubbing; rake makes it cut
A lathe tool bit has two kinds of angle. Relief (also called clearance) is ground under the cutting edge so the tool’s side and front don’t rub on the work: side relief under the side edge, front relief under the end. Rake is ground on top, sloping away from the edge, so the chip slides off instead of being pushed: side rake across the top, back rake along it.
Rake and relief together set the wedge, or keenness, angle: 90° less the side rake and the side relief. A thin wedge cuts soft metal easily but chips in hard metal; a blunt wedge is strong but pushes. The Army’s table gives machine steel 12–18° side rake and 10–12° side relief, a 60–68° wedge, and South Bend says about 60° for mild steel and 80–85° for cast iron and hard steel.
Why the material changes the tool
Soft, gummy metals want a keen edge and a lot of rake so the chip flows: the Army’s table gives aluminum 15° side rake and 35° back rake. Brass and bronze are the opposite. A raked tool pulls itself into them and grabs, so they get almost none: 5° to −4° side rake and 0° back rake, a tool ground flat on top.
Cast iron and tool steel sit between, with modest rake (12° side) to keep the edge strong. The relief barely changes across the table, 10–12° at the side and 8–10° at the front, because its job (not rubbing) is the same in every material.
The cutting-edge angles and the nose
Seen from above, the side cutting edge is angled back from the bit’s side and the end cutting edge back from square. The Navy’s manual recommends about 15° for each in rough turning: the side angle spreads the cut along more edge and thins the chip, and the end angle keeps the tool’s heel from dragging on the finished surface. Grind 0° on the side when the tool must cut up to a square shoulder.
A small radius on the nose, 1/64 to 1/32 inch, makes the point last and leaves a better finish. Too big a radius chatters.
Grinding it
South Bend’s order for a right-hand turning tool: grind the left side (the side cutting edge and its relief), then the right side, then the front (the end cutting edge and its relief), round the nose, grind the top for side and back rake, and hone the edge with an oilstone. Keep the bit moving across the wheel and dip it in water often; a bit too hot to hold is too hot.
A parting tool has no side rake and clearance down both sides of the blade. A threading tool is a 60° point checked in a centre gauge and left flat on top, because any rake changes the angle it cuts. Both go exactly on centre height.
At the grinder, grind on the face of the wheel, with the tool rest close to it.
Try it on a calculator
- HSS lathe tool grinding — The rake, relief and cutting-edge angles to grind a high-speed steel lathe tool for your material, with the tool drawn and the grinding order.
- Turning speeds and feeds calculator — Material, insert and setup to speed, feed, DOC, RPM and G-code.
- Single-point threading calculator — Thread depth, compound setting, passes and infeed, the thread dial for your lathe, a G76 line for Fanuc or Haas, and the wire check.
Charts
- Lathe tool angles — Side and front relief, side and back rake for a hand-ground HSS tool, by material, from the US Army’s machinist manual.
Check yourself: 5 questions
Check yourself
0 of 5 answered