Lathe
HSS lathe tool grinding
Rake, relief and edge angles to grind a high-speed steel lathe tool for your material.
For a hand-ground high-speed steel tool bit.
Right-hand turning tool for machine steel
| Angle | Grind |
|---|---|
| Side relief | 10–12°One source: US Army TC 9-524, the military’s machinist training manual |
| Front (end) relief | 8°One source: US Army TC 9-524, the military’s machinist training manual |
| Side rake | 12–18°One source: US Army TC 9-524, the military’s machinist training manual |
| Back rake | 8–15°One source: US Army TC 9-524, the military’s machinist training manual |
| Side cutting edge angle0° to cut up to a square shoulder; up to 30° | 15°US Navy Machinery Repairman manual, general figure for turning tools |
| End cutting edge angle8–30° in use; a little more for finishing | 15°US Navy Machinery Repairman manual, general figure for turning tools |
| Wedge (keenness) angle | 60–68°Geometry: 90° less the side rake and side relief |
| Nose radius | 1/64–1/32" (0.4–0.8 mm)US Navy Machinery Repairman manual, general figure for turning tools |
The tool, drawn from these angles
Where the table gives a range, the drawing uses its middle. Not to scale.
Grinding order
- Grind the left side: the side cutting edge at 15° to the bit's side, with 10–12° side relief under it.
- Grind the right side back far enough to clear the work.
- Grind the front: the end cutting edge at 15°, with 8° front relief under it.
- Round the nose to 1/64–1/32" radius where the two edges meet.
- Grind the top: 12–18° side rake falling away from the cutting edge, and 8–15° back rake.
- Hone the cutting edge with an oilstone.
Dip the bit in water often: if it gets too hot to hold, it's too hot. The order follows South Bend's How to Run a Lathe.
What next
What speed and feed for this lathe cut?Lathe SFM, feed and depth of cut for your material and insert, with the RPM.
How deep, and how many passes, for this thread?Thread depth, compound setting, infeed per pass and a G76 line for lathe threading.
What’s wrong with this cut?Stringy chips, chatter, a torn finish, built-up edge or chipped inserts: causes and what to change.
How the hSS lathe tool grinding works
For machine steel, grind a high-speed steel turning tool with 10–12° side relief, 8° front relief, 12–18° side rake and 8–15° back rake (US Army TC 9-524), and 15° side and end cutting-edge angles with a 1/64–1/32" nose (US Navy). Pick your tool and material for the rest.
More
- Lathe tool angle chart: all eight materials side by side
- Lesson: Grinding a HSS lathe tool: what each angle does
- Turning speeds & feeds: HSS speeds for your material
Sources
- US Army TC 9-524, Fundamentals of Machine Tools, Table 7-1: tool bit angles by material
- US Navy, Machinery Repairman 3 & 2 (NAVEDTRA, 1990), chapter 6: cutting tool angles
- South Bend Lathe Works, How to Run a Lathe (1934): grinding lathe tool cutter bits
The Army's table is the one per-material table we could read; Little Machine Shop's sheet reprints it. The drawings are ours.