End mills
Chip loads and speeds for carbide end mills, with fixes for chatter and breakage.
When an end mill goes in the turret, I check its length offset against the setup sheet before the first part. The program does exactly what the offset tells it.
Quick numbers
For a 1/2 in solid carbide end millAluminum, chip load.0036"Median of 5 makers. Middle half .0026"–.0041"; all .0022"–.0042"
Carbon steel, chip load.0025"Median of 7 makers. Middle half .0023"–.0028"; all .0011"–.0030"
304 and 316 stainless, chip load.0018"Median of 7 makers. Middle half .0015"–.0023"; all .0009"–.0035"
Aluminum, speed600 SFMMedian of 5 makers. Middle half 550–925; all 400–1,500
Carbon steel, speed328 SFMMedian of 8 makers. Middle half 225–368; all 100–620
304 and 316 stainless, speed293 SFMMedian of 8 makers. Middle half 219–318; all 100–380
Calculators
- Milling speeds and feeds calculatorEnd mill, material and cut to RPM, chip load and IPM, with chip thinning.
- Chip load and feed rate calculatorRPM, flutes and chip load to IPM, or back to chip load or RPM, with chip thinning.
- Ramp angle and helix calculatorRamp angle to Z per turn for a helical entry, turns to depth and the centre feed; straight ramps too.
- Thread milling calculatorA ready helical thread-milling program for UN and metric threads, inside or out: climb direction, radial passes, corrected feed and comp.
Fix a problem
- Chatter and vibrationA squeal or hum, and a wavy, washboard pattern on the floor or walls. Worst with long tools, thin walls and in corners.
- Tapered walls or parts out of sizeWalls lean or come out thick at the bottom, sizes change from pass to pass, or a spring pass still takes metal. The tool is bending.
- Rough or torn finishFeed marks you can feel, torn or smeared spots, or a dull, rough floor where the print wants a clean finish.
- End mill or insert breaksThe tool snaps or a whole corner breaks out, often all at once: at the start of a cut, in a slot, or as it wears.
- Chipped or notched edgesSmall chips missing along the edge or corner, cracks across the edge, or a notch worn in at the depth-of-cut line.
- Built-up edgeMetal welds onto the cutting edge, then breaks off and takes edge with it. A smeared finish; common in aluminum, stainless and soft steel.
- Chips recut or packing the flutesChips pile up in a slot or pocket and get cut again: scratched floors, a crunching sound, chips welded into the flutes.
Charts
Guides
Sources
Sources8
- Harvey Tool — General machining guidelines, carbide end mills (SFM and chip load by diameter) (archived May 13, 2026)
- 6G Tools — Carbide end mill speeds and feeds, general purpose: AlTiN coated (steel, stainless, iron, heat-resistant) and uncoated (non-ferrous) (archived Mar 11, 2026)
- RedLine Tools — General purpose carbide end mills (catalog pp. 215–216) and 5-flute aluminum end mills, slotting (p. 188) (archived May 29, 2022)
- Amana Tool — Solid carbide ZrN square aluminum end mills (3 flute, slotting 1 × D) and AlTiN miniature end mills for steel, stainless and composites (1 × D) (archived Nov 12, 2026)
- Niagara Cutter (a Seco Tools company) — Catalog & technical guide: general purpose solid carbide C430 (4 flute) and C330 (3 flute), slotting start values (pp. 200, 207) (archived Nov 13, 2026)
- Maritool — Speeds and feeds for 1001 and 1002 series end mills (solid carbide, 4 flute, TiAlN) (archived Apr 20, 2021)
- Kyocera SGS — Z-Carb HPR (Series Z5, Z5CR) speed and feed recommendations, fractional, slot rows (archived Oct 7, 2024)
- Kennametal — GOmill GP general purpose solid carbide end mills, 4SE..IS-IR, KC633M: application data (catalog p. B224) (archived Nov 11, 2026)