Class 1500 spiral wound gasket dimensions

A Class 1500 NPS 2 spiral wound gasket winds from 2.31" to 3.38" on a 5.63" centering ring. The four diameters of a spiral wound gasket with inner and centering rings, NPS 1/2 to 24. Each is checked against three published copies of the standard (two for the inner ring); a tag marks any size where they differ.

The Class 1500 NPS 2 spiral wound gasket, face on, to scale: centering ring Ø5.63", winding Ø2.31"–3.38".centering ring Ø5.63"winding Ø2.31"–3.38"
The Class 1500 NPS 2 spiral wound gasket, face on. To scale.
Units

Class 1500 spiral wound gasket chart

Class 1500 spiral wound gaskets: inner ring ID, winding ID and OD, centering ring OD by pipe size
NPSInner ring ID (inmm)Winding ID (inmm)Winding OD (inmm)Centering ring OD (inmm)Inner ring
1/20.5614.20.7519.11.2531.82.5063.5Not required
3/40.8120.61.0025.41.5639.72.7569.9Not required
11.0626.91.2531.81.8847.63.1379.4Not required
1-1/41.3133.31.5639.72.3860.33.5088.9Not required
1-1/21.6341.41.8847.62.7569.93.8898.4Not required
22.0652.32.3158.73.3885.75.63142.9Not required
2-1/22.5063.52.7569.93.8898.46.50165.1Not required
33.1078.73.6392.14.75120.76.88174.6Not required
43.8597.84.63117.55.88149.28.25209.6Not required
54.90124.55.63142.97.00177.810.00254.0Not required
65.80147.36.75171.58.25209.611.13282.6Not required
87.75196.98.50215.910.13257.213.88352.4Not required
109.69246.110.50266.712.25311.217.13435.0Not required
1211.50292.112.75323.914.50368.320.50520.7Required
1412.63320.814.25362.015.75400.122.75577.9Required
1614.50368.316.00406.418.00457.225.25641.4Required
1816.75425.518.25463.620.50520.727.75704.9Required
2018.75476.320.25514.422.50571.529.75755.7Required
2422.75577.924.25616.026.75679.535.50901.7Required

Per ASME B16.20, checked against Lamons, Flexitallic and APG. Winding 0.175" (4.45 mm) thick; rings 0.117–0.131". breakingchips.com/gaskets/spiral-wound/class-1500/

Thickness

Show
Winding
0.175" (4.45 mm), uncompressed
Inner and centering rings
0.117–0.131" (2.97–3.33 mm), nominally 1/8"

The rings stop the winding crushing: the joint is made up when the flanges close on them. Winding: Flexitallic and Wermac; ring range: Lamons and Wermac.

When the inner ring is required

Show
  • Class 900 NPS 24, Class 1500 NPS 12–24 and Class 2500 NPS 4–12 (on this chart: NPS 12, 14, 16, 18, 20, 24).
  • Any PTFE-filled winding, at every size.
  • Flexitallic also fits one to every flexible graphite gasket unless the buyer says not to.

Elsewhere it is optional, though many makers fit one by default: it keeps the winding from buckling inward and smooths the flow past the joint. Lamons, Flexitallic and APG all print these rules.

Sources

Sources5