ASME B16.5 · Class 600 (600#)

1-1/4" Class 600 flange: bolts and torque

A 1-1/4" Class 600 flange takes 4 studs, 5/8-11 UNC, on a 3-7/8" bolt circle, 3-3/4" long for a raised face and 3-3/4" for a ring joint. With a spiral wound gasket and B7 studs the gasket makers' tables give 85.5 ft·lb per stud.

A Class 600 NPS 1-1/4 flange face on, to scale: 5-1/4" OD, 4 holes of 3/4" on a 3-7/8" bolt circle, each with a 5/8" stud.OD 5-1/4"bolt circle 3-7/8"hole 4 × 3/4"bolt 4 × 5/8"
The NPS 1-1/4 Class 600 flange, face on. To scale.

A starting point from published gasket-maker tables. Your site’s bolting procedure, or a PCC-1 qualified joint procedure, governs pressure piping.

Studs and flange

Studs
4 × 5/8-11 UNC
Stud length, raised face
3-3/4" (1/4" raised face)
Stud length, ring joint
3-3/4"
Nut wrench
1-1/16" (heavy hex)
Bolt circle
3-7/8"
Flange OD
5-1/4"
Bolt holes
3/4"

Checked against 3 published copies

Stud lengths are measured first thread to first thread, as B16.5 lists them.

Torque by gasket

Per stud, ASTM A193 B7 studs with 2H nuts, lubricated as each maker's table assumes.

  • Spiral wound85.5 ft·lb · 116 N·m

    Garlock 120 · Flexitallic 70 · Teadit 85 · FNW 86 ft·lb (span 41–120)

    Median of 4 makers

  • Sheet (PTFE, graphite, fibre)

    Not shown: Sheet gasket makers publish torque only for Class 150 and 300 flanges; above that they say to ask them.

  • Ring joint (RTJ)99.3 ft·lb · 135 N·m

    Computed, no maker table: no gasket maker prints ring joint torque per flange size.

    How it's computed

    T = K × D × F at 60% of B7 yield (63 ksi) on the .202 in² root area, K 0.15.

Median of 4 makers

Work it in the calculator: other stud materials (B7M, L7, B8M), your lubricant's K, or your own bolt stress.

Passes (spiral wound, 85.5 ft·lb)

Passes for the spiral wound gasket, to 85.5 ft·lb
  1. Snug by hand, then a short wrench, in the star
  2. 30% in the star25.7 ft·lb
  3. 60–70% in the star51.3–59.9 ft·lb
  4. 100% in the star85.5 ft·lb
  5. Check bolt to bolt round the flange until no nut turns85.5 ft·lb

The passes as the gasket makers print them.

Tightening order for 4 bolts →

Gaskets for this flange

Spiral wound, sheet and ring joint sizes

Dimensions from ASME B16.20 (spiral wound, ring joint) and B16.21 (sheet), checked against published copies.

Units
Spiral wound
Inner ring ID1.5038.1
Winding ID × OD1.8847.6 × 2.3860.3
Centering ring OD3.2582.6
Inner ringNot required
Sheet ring
ID × OD1.6642.2 × 3.2582.6
Ring joint
Ring numberR-18

Sources

Sources10