ASME B16.21 · non-metallic flat gaskets for ASME B16.5 flanges

Class 600 gasket dimensions

A Class 600 NPS 2 sheet gasket is 2.38" ID × 4.38" OD. Cut sizes for compressed fibre, PTFE, graphite and rubber sheet gaskets. A ring gasket sits inside the bolts on a raised face. Each size is checked against three or four published copies of the standard; a tag marks any that differ.

The Class 600 NPS 2 sheet gasket, face on, to scale: size value 2.38" ID × 4.38" OD.2.38" ID × 4.38" OD
The Class 600 NPS 2 sheet gasket, face on. To scale.
Units

Class 600 sheet gasket chart

Class 600 ring gaskets by pipe size
NPSID (inmm)Ring OD (inmm)
1/20.8421.32.1253.8
3/41.0626.92.6266.5
11.3133.32.8873.2
1-1/41.6642.23.2582.6
1-1/21.9148.53.7595.3
22.3860.54.38111.3
2-1/22.8873.25.12130.0
33.5088.95.88149.4
3-1/24.00101.66.38162.1
44.50114.37.62193.5
55.56141.29.50241.3
66.62168.110.50266.7
88.62218.912.62320.5
1010.75273.115.75400.1
1212.75323.918.00457.2
1414.00355.619.38492.3
1616.00406.422.25565.2
1818.00457.224.12612.6
2020.00508.026.88682.8
2424.00609.631.12790.4

Per ASME B16.21, checked against Garlock, Lamons, AmesWeb and Wermac. B16.21 sets the cut diameters, not the thickness. breakingchips.com/gaskets/sheet/class-600/

Before you cut

The ID, higher classes and full-face sizes
  • The ID is the pipe’s outside diameter (0.84" at NPS 1/2), so it is the same in every class; the OD changes with the bolt circle.
  • Garlock notes that non-metallic gaskets are normally used on Class 150 and 300 flanges: check the service conditions with the gasket maker.
  • B16.21 lists no sheet gaskets above Class 900. For Class 1500 and 2500 use a spiral wound or ring joint gasket.
  • Full-face sizes are given here for Class 150 and 300 only: Garlock notes B16.21 gives none above Class 300.

Sources

Sources5