ASTM E140 · Non-austenitic steel

33 HRC to HV and HB (ASTM E140)

By ASTM E140 Table 1, 33 HRC equals 327 HV (Vickers) and 311 HB (Brinell, 10 mm carbide ball), for carbon, alloy and tool steel. Conversions are approximate; austenitic stainless, cast iron and nonferrous metals need other tables.

33 HRC on the three scales: 311 HB and 327 HV, as ASTM E140 converts it.HRCHBHVHRC 33HB 311HV 3272025304550556065400500600700300400500600700900
33 HRC across the ASTM E140 scales. The scales aligned by E140’s conversion rows; they are not linear against each other.
Brinell
311 HB

10 mm carbide ball, 3000 kgf (HBW)

Vickers
327 HV

Checked against 5 published copies

Nearby values

Other sizes
Rockwell C 30 to 36 in Vickers and Brinell
HRCHVHB
30 HRC302286
31 HRC310294
32 HRC318301
33 HRC327311
34 HRC336319
35 HRC345327
36 HRC354336

Sources

Sources5