ASTM E140 · Non-austenitic steel
30 HRC to HV and HB (ASTM E140)
By ASTM E140 Table 1, 30 HRC equals 302 HV (Vickers) and 286 HB (Brinell, 10 mm carbide ball), for carbon, alloy and tool steel. Conversions are approximate; austenitic stainless, cast iron and nonferrous metals need other tables.
- Brinell
- 286 HB
10 mm carbide ball, 3000 kgf (HBW)
- Vickers
- 302 HV
Checked against 5 published copies
Nearby values
Sources
Sources5
ASTM E140, Standard Hardness Conversion Tables for Metals, Tables 1 and 2 (non-austenitic steels). Every value on this page was checked against these published copies:
- Phase II — Rockwell C hardness conversion chart (ASTM E140 Table 1) (archived May 13, 2026)
- LabTesting — Rockwell C hardness conversion, non-austenitic steels (archived Jul 13, 2026)
- NSM — Hardness conversion calculator (ASTM E140 Tables 1 and 2) (archived Nov 16, 2026)
- Misumi — Conversion table of hardness, SAE J417 (from ASTM E140 Table 1) (archived Nov 15, 2026)
- Honesdom (hardnessgauge.com) — Hardness conversion chart, Rockwell C (archived May 15, 2026)