ASTM E140 · Non-austenitic steel

36 HRC to HV and HB (ASTM E140)

By ASTM E140 Table 1, 36 HRC equals 354 HV (Vickers) and 336 HB (Brinell, 10 mm carbide ball), for carbon, alloy and tool steel. Conversions are approximate; austenitic stainless, cast iron and nonferrous metals need other tables.

36 HRC on the three scales: 336 HB and 354 HV, as ASTM E140 converts it.HRCHBHVHRC 36HB 336HV 35420253050556065300500600700300400500600700900
36 HRC across the ASTM E140 scales. The scales aligned by E140’s conversion rows; they are not linear against each other.
Brinell
336 HB

10 mm carbide ball, 3000 kgf (HBW)

Vickers
354 HV

Checked against 5 published copies

Nearby values

Other sizes
Rockwell C 33 to 39 in Vickers and Brinell
HRCHVHB
33 HRC327311
34 HRC336319
35 HRC345327
36 HRC354336
37 HRC363344
38 HRC372353
39 HRC382362

Sources

Sources5