ASTM E140 · Non-austenitic steel

39 HRC to HV and HB (ASTM E140)

By ASTM E140 Table 1, 39 HRC equals 382 HV (Vickers) and 362 HB (Brinell, 10 mm carbide ball), for carbon, alloy and tool steel. Conversions are approximate; austenitic stainless, cast iron and nonferrous metals need other tables.

39 HRC on the three scales: 362 HB and 382 HV, as ASTM E140 converts it.HRCHBHVHRC 39HB 362HV 3822025303550556065300500600700300500600700900
39 HRC across the ASTM E140 scales. The scales aligned by E140’s conversion rows; they are not linear against each other.
Brinell
362 HB

10 mm carbide ball, 3000 kgf (HBW)

Vickers
382 HV

Checked against 5 published copies

Nearby values

Other sizes
Rockwell C 36 to 42 in Vickers and Brinell
HRCHVHB
36 HRC354336
37 HRC363344
38 HRC372353
39 HRC382362
40 HRC392371
41 HRC402381
42 HRC412390

Sources

Sources5