ASTM E140 · Non-austenitic steel

46 HRC to HV and HB (ASTM E140)

By ASTM E140 Table 1, 46 HRC equals 458 HV (Vickers) and 432 HB (Brinell, 10 mm carbide ball), for carbon, alloy and tool steel. Conversions are approximate; austenitic stainless, cast iron and nonferrous metals need other tables.

46 HRC on the three scales: 432 HB and 458 HV, as ASTM E140 converts it.HRCHBHVHRC 46HB 432HV 45820253035406065300400600700300400500600700900
46 HRC across the ASTM E140 scales. The scales aligned by E140’s conversion rows; they are not linear against each other.
Brinell
432 HB

10 mm carbide ball, 3000 kgf (HBW)

Vickers
458 HV

Checked against 5 published copies

Nearby values

Other sizes
Rockwell C 43 to 49 in Vickers and Brinell
HRCHVHB
43 HRC423400
44 HRC434409
45 HRC446421
46 HRC458432
47 HRC471443
48 HRC484455
49 HRC498469

Sources

Sources5