ASTM E140 · Non-austenitic steel

43 HRC to HV and HB (ASTM E140)

By ASTM E140 Table 1, 43 HRC equals 423 HV (Vickers) and 400 HB (Brinell, 10 mm carbide ball), for carbon, alloy and tool steel. Conversions are approximate; austenitic stainless, cast iron and nonferrous metals need other tables.

43 HRC on the three scales: 400 HB and 423 HV, as ASTM E140 converts it.HRCHBHVHRC 43HB 400HV 4232025303540556065300600700300400500600700900
43 HRC across the ASTM E140 scales. The scales aligned by E140’s conversion rows; they are not linear against each other.
Brinell
400 HB

10 mm carbide ball, 3000 kgf (HBW)

Vickers
423 HV

Checked against 5 published copies

Nearby values

Other sizes
Rockwell C 40 to 46 in Vickers and Brinell
HRCHVHB
40 HRC392371
41 HRC402381
42 HRC412390
43 HRC423400
44 HRC434409
45 HRC446421
46 HRC458432