ASTM E140 · Non-austenitic steel
63 HRC to HV and HB (ASTM E140)
By ASTM E140 Table 1, 63 HRC equals 772 HV (Vickers) and 705 HB (Brinell, 10 mm carbide ball; E140 prints it in parentheses, above Brinell’s 650 limit), for carbon, alloy and tool steel. Conversions are approximate; austenitic stainless, cast iron and nonferrous metals need other tables.
- Brinell
- (705) HB
10 mm carbide ball, 3000 kgf (HBW). In parentheses: above 650, past Brinell’s recommended range
- Vickers
- 772 HV
Checked against 4 published copies
Nearby values
Sources
Sources5
ASTM E140, Standard Hardness Conversion Tables for Metals, Tables 1 and 2 (non-austenitic steels). Every value on this page was checked against these published copies:
- Phase II — Rockwell C hardness conversion chart (ASTM E140 Table 1) (archived May 13, 2026)
- LabTesting — Rockwell C hardness conversion, non-austenitic steels (archived Jul 13, 2026)
- NSM — Hardness conversion calculator (ASTM E140 Tables 1 and 2) (archived Nov 16, 2026)
- Misumi — Conversion table of hardness, SAE J417 (from ASTM E140 Table 1) (archived Nov 15, 2026)
- Honesdom (hardnessgauge.com) — Hardness conversion chart, Rockwell C (archived May 15, 2026)