AS568 · 0 series

AS568-038 O-ring size

AS568-038 is 2.614" ID × 0.070" cross section (66.40 × 1.78 mm), held to ± 0.020" and ± 0.003", 2.754" OD, checked against 3 published copies. For a static radial seal, cut the groove 0.050–0.055" deep and 0.093–0.110" wide (Parker and Apple Rubber).

A 0.070" O-ring cross section in a static radial gland, in section: squeezed between the groove bottom and the bore, its free section dashed over it.free section 0.070"squeeze 18–32 %boreO-ringgland depth 0.050–0.055"gland width 0.093–0.110"piston
AS568-038 in a static radial gland. Drawn to scale at the gland’s middle depth and width.

Size and tolerances

Inside diameter
2.614 ± 0.020" (66.40 mm)
Cross section
0.070 ± 0.003" (1.78 mm)
Outside diameter
2.754" (ID + 2 × cross section)

Two published copies agree

AS568 sizes are nominal inch sizes; the tolerances are the ones the copies print. The first digit of the dash number is the cross-section series, so every 0 series ring shares this cross section.

Groove for a 0.070" cross section

Depth and width as a range spanning Parker’s and Apple Rubber’s gland tables. For the bore and gland diameters, use the groove calculator.

Gland depth and width for AS568-038, by seal type
SealDepthWidth
Static radial (piston or rod)0.050–0.055"0.093–0.110"
Face seal0.049–0.054"0.100–0.110"
Dynamic (reciprocating)0.055–0.057"0.090–0.100"

Only two makers publish this: Parker and Apple Rubber