O-ring size chart (AS568)

Every standard AS568 O-ring, -004 to -475, with its inside diameter and cross section in inches and mm, and a page for each. Read a dash number by its first digit, the cross section: -0xx is 0.070", -1xx 0.103", -2xx 0.139", -3xx 0.210" and -4xx 0.275". The last two digits step the inside diameter up within that section. The finder gives the nearest AS568 size to a metric O-ring.

Inside diameter and cross section for every standard AS568 dash size, with tolerances, as three O-ring makers print the standard; a value carries a tag only where the copies differ. The first digit of the dash number is the cross-section series. To cut the groove, see the O-ring groove chart.

Nearest AS568 to a metric O-ring

Type the metric size. The nearest AS568 cross section comes first, then the nearest inside diameters in it; a ring a little off on ID stretches or squeezes to fit, but the cross section sets the groove.

    0 series (1/16" nominal cross section)

    AS568 0 series: inside diameter, cross section and outside diameter
    DashIDCross sectionID × CS, mmOD
    -0040.070 ± 0.005"Only one published copy——
    -0050.101 ± 0.005"0.070 ± 0.003"2.57 × 1.780.241"
    -0060.114 ± 0.005"0.070 ± 0.003"2.90 × 1.780.254"
    -0070.145 ± 0.005"0.070 ± 0.003"3.68 × 1.780.285"
    -0080.176 ± 0.005"0.070 ± 0.003"4.47 × 1.780.316"
    -0090.208 ± 0.005"0.070 ± 0.003"5.28 × 1.780.348"
    -0100.239 ± 0.005"0.070 ± 0.003"6.07 × 1.780.379"
    -0110.301 ± 0.005"0.070 ± 0.003"7.65 × 1.780.441"
    -0120.364 ± 0.005"0.070 ± 0.003"9.25 × 1.780.504"
    -0130.426 ± 0.005"0.070 ± 0.003"10.82 × 1.780.566"
    -0140.489 ± 0.005"0.070 ± 0.003"12.42 × 1.780.629"
    -0150.551 ± 0.007"0.070 ± 0.003"14.00 × 1.780.691"
    -0160.614 ± 0.009"0.070 ± 0.003"15.60 × 1.780.754"
    -0170.676 ± 0.009"0.070 ± 0.003"17.17 × 1.780.816"
    -0180.739 ± 0.009"0.070 ± 0.003"18.77 × 1.780.879"
    -0190.801 ± 0.009"0.070 ± 0.003"20.35 × 1.780.941"
    -0200.864 ± 0.009"0.070 ± 0.003"21.95 × 1.781.004"
    -0210.926 ± 0.009"0.070 ± 0.003"23.52 × 1.781.066"
    -0220.989 ± 0.010"0.070 ± 0.003"25.12 × 1.781.129"
    -0231.051 ± 0.010"0.070 ± 0.003"26.70 × 1.781.191"
    -0241.114 ± 0.010"0.070 ± 0.003"28.30 × 1.781.254"
    -0251.176 ± 0.011"0.070 ± 0.003"29.87 × 1.781.316"
    -0261.239 ± 0.011"0.070 ± 0.003"31.47 × 1.781.379"
    -0271.301 ± 0.011"0.070 ± 0.003"33.05 × 1.781.441"
    -0281.364 ± 0.013"0.070 ± 0.003"34.65 × 1.781.504"
    -0291.489 ± 0.013"0.070 ± 0.003"37.82 × 1.781.629"
    -0301.614 ± 0.013"0.070 ± 0.003"41.00 × 1.781.754"
    -0311.739 ± 0.015"0.070 ± 0.003"44.17 × 1.781.879"
    -0321.864 ± 0.015"0.070 ± 0.003"47.35 × 1.782.004"
    -0331.989 ± 0.018"0.070 ± 0.003"50.52 × 1.782.129"
    -0342.114 ± 0.018"0.070 ± 0.003"53.70 × 1.782.254"
    -0352.239 ± 0.018"0.070 ± 0.003"56.87 × 1.782.379"
    -0362.364 ± 0.018"0.070 ± 0.003"60.05 × 1.782.504"
    -0372.489 ± 0.018"0.070 ± 0.003"63.22 × 1.782.629"
    -0382.614 ± 0.020"0.070 ± 0.003"66.40 × 1.782.754"
    -0392.739 ± 0.020"0.070 ± 0.003"69.57 × 1.782.879"
    -0402.864 ± 0.020"0.070 ± 0.003"72.75 × 1.783.004"
    -0412.989 ± 0.024"0.070 ± 0.003"75.92 × 1.783.129"
    -0423.239 ± 0.024"0.070 ± 0.003"82.27 × 1.783.379"
    -0433.489 ± 0.024"0.070 ± 0.003"88.62 × 1.783.629"
    -0443.739 ± 0.027"0.070 ± 0.003"94.97 × 1.783.879"
    -0453.989 ± 0.027"0.070 ± 0.003"101.32 × 1.784.129"
    -0464.239 ± 0.030"0.070 ± 0.003"107.67 × 1.784.379"
    -0474.489 ± 0.030"0.070 ± 0.003"114.02 × 1.784.629"
    -0484.739 ± 0.030"0.070 ± 0.003"120.37 × 1.784.879"
    -0494.989 ± 0.037"0.070 ± 0.003"126.72 × 1.785.129"
    -0505.239 ± 0.037"0.070 ± 0.003"133.07 × 1.785.379"

    100 series

    AS568 100 series: inside diameter, cross section and outside diameter
    DashIDCross sectionID × CS, mmOD
    -1020.049 ± 0.005" or 0.049 ± 0.004"

    Two charts disagree: Freudenberg-Simrit and Global O-Ring 0.049 ± 0.005", Greene Tweed 0.049 ± 0.004"

    0.103 ± 0.003"——
    -1030.081 ± 0.005"0.103 ± 0.003"2.06 × 2.620.287"
    -1040.112 ± 0.005"0.103 ± 0.003"2.84 × 2.620.318"
    -1050.143 ± 0.005"0.103 ± 0.003"3.63 × 2.620.349"
    -1060.174 ± 0.005"0.103 ± 0.003"4.42 × 2.620.380"
    -1070.206 ± 0.005"0.103 ± 0.003"5.23 × 2.620.412"
    -1080.237 ± 0.005"0.103 ± 0.003"6.02 × 2.620.443"
    -1090.299 ± 0.005"0.103 ± 0.003"7.59 × 2.620.505"
    -1100.362 ± 0.005"0.103 ± 0.003"9.19 × 2.620.568"
    -1110.424 ± 0.005"0.103 ± 0.003"10.77 × 2.620.630"
    -1120.487 ± 0.005"0.103 ± 0.003"12.37 × 2.620.693"
    -1130.549 ± 0.007"0.103 ± 0.003"13.94 × 2.620.755"
    -1140.612 ± 0.009"0.103 ± 0.003"15.54 × 2.620.818"
    -1150.674 ± 0.009"0.103 ± 0.003"17.12 × 2.620.880"
    -1160.737 ± 0.009"0.103 ± 0.003"18.72 × 2.620.943"
    -1170.799 ± 0.010"0.103 ± 0.003"20.29 × 2.621.005"
    -1180.862 ± 0.010"0.103 ± 0.003"21.89 × 2.621.068"
    -1190.924 ± 0.010"0.103 ± 0.003"23.47 × 2.621.130"
    -1200.987 ± 0.010"0.103 ± 0.003"25.07 × 2.621.193"
    -1211.049 ± 0.010"0.103 ± 0.003"26.64 × 2.621.255"
    -1221.112 ± 0.010"0.103 ± 0.003"28.24 × 2.621.318"
    -1231.174 ± 0.012"0.103 ± 0.003"29.82 × 2.621.380"
    -1241.237 ± 0.012"0.103 ± 0.003"31.42 × 2.621.443"
    -1251.299 ± 0.012"0.103 ± 0.003"32.99 × 2.621.505"
    -1261.362 ± 0.012"0.103 ± 0.003"34.59 × 2.621.568"
    -1271.424 ± 0.012"0.103 ± 0.003"36.17 × 2.621.630"
    -1281.487 ± 0.012"0.103 ± 0.003"37.77 × 2.621.693"
    -1291.549 ± 0.015"0.103 ± 0.003"39.34 × 2.621.755"
    -1301.612 ± 0.015"0.103 ± 0.003"40.94 × 2.621.818"
    -1311.674 ± 0.015"0.103 ± 0.003"42.52 × 2.621.880"
    -1321.737 ± 0.015"0.103 ± 0.003"44.12 × 2.621.943"
    -1331.799 ± 0.015"0.103 ± 0.003"45.69 × 2.622.005"
    -1341.862 ± 0.015"0.103 ± 0.003"47.29 × 2.622.068"
    -1351.925 ± 0.017"0.103 ± 0.003"48.90 × 2.622.131"
    -1361.987 ± 0.017"0.103 ± 0.003"50.47 × 2.622.193"
    -1372.050 ± 0.017"0.103 ± 0.003"52.07 × 2.622.256"
    -1382.112 ± 0.017"0.103 ± 0.003"53.64 × 2.622.318"
    -1392.175 ± 0.017"0.103 ± 0.003"55.25 × 2.622.381"
    -1402.237 ± 0.017"0.103 ± 0.003"56.82 × 2.622.443"
    -1412.300 ± 0.020"0.103 ± 0.003"58.42 × 2.622.506"
    -1422.362 ± 0.020"0.103 ± 0.003"59.99 × 2.622.568"
    -1432.425 ± 0.020"0.103 ± 0.003"61.60 × 2.622.631"
    -1442.487 ± 0.020"0.103 ± 0.003"63.17 × 2.622.693"
    -1452.550 ± 0.020"0.103 ± 0.003"64.77 × 2.622.756"
    -1462.612 ± 0.020"0.103 ± 0.003"66.34 × 2.622.818"
    -1472.675 ± 0.022"0.103 ± 0.003"67.95 × 2.622.881"
    -1482.737 ± 0.022"0.103 ± 0.003"69.52 × 2.622.943"
    -1492.800 ± 0.022"0.103 ± 0.003"71.12 × 2.623.006"
    -1502.862 ± 0.022"0.103 ± 0.003"72.69 × 2.623.068"
    -1512.987 ± 0.024"0.103 ± 0.003"75.87 × 2.623.193"
    -1523.237 ± 0.024"0.103 ± 0.003"82.22 × 2.623.443"
    -1533.487 ± 0.024"0.103 ± 0.003"88.57 × 2.623.693"
    -1543.737 ± 0.028"0.103 ± 0.003"94.92 × 2.623.943"
    -1553.987 ± 0.028"0.103 ± 0.003"101.27 × 2.624.193"
    -1564.237 ± 0.030"0.103 ± 0.003"107.62 × 2.624.443"
    -1574.487 ± 0.030"0.103 ± 0.003"113.97 × 2.624.693"
    -1584.737 ± 0.030"0.103 ± 0.003"120.32 × 2.624.943"
    -1594.987 ± 0.035"0.103 ± 0.003"126.67 × 2.625.193"
    -1605.237 ± 0.035"0.103 ± 0.003"133.02 × 2.625.443"
    -1615.487 ± 0.035"0.103 ± 0.003"139.37 × 2.625.693"
    -1625.737 ± 0.035"0.103 ± 0.003"145.72 × 2.625.943"
    -1635.987 ± 0.035"0.103 ± 0.003"152.07 × 2.626.193"
    -1646.237 ± 0.040"0.103 ± 0.003"158.42 × 2.626.443"
    -1656.487 ± 0.040"0.103 ± 0.003"164.77 × 2.626.693"
    -1666.737 ± 0.040"0.103 ± 0.003"171.12 × 2.626.943"
    -1676.987 ± 0.040"0.103 ± 0.003"177.47 × 2.627.193"
    -1687.237 ± 0.045"0.103 ± 0.003"183.82 × 2.627.443"
    -1697.487 ± 0.045"0.103 ± 0.003"190.17 × 2.627.693"
    -1707.737 ± 0.045"0.103 ± 0.003"196.52 × 2.627.943"
    -1717.987 ± 0.045"0.103 ± 0.003"202.87 × 2.628.193"
    -1728.237 ± 0.050"0.103 ± 0.003"209.22 × 2.628.443"
    -1738.487 ± 0.050"0.103 ± 0.003"215.57 × 2.628.693"
    -1748.737 ± 0.050"0.103 ± 0.003"221.92 × 2.628.943"
    -1758.987 ± 0.050"0.103 ± 0.003"228.27 × 2.629.193"
    -1769.237 ± 0.055"0.103 ± 0.003"234.62 × 2.629.443"
    -1779.487 ± 0.055"0.103 ± 0.003"240.97 × 2.629.693"
    -1789.737 ± 0.055"0.103 ± 0.003"247.32 × 2.629.943"

    200 series

    AS568 200 series: inside diameter, cross section and outside diameter
    DashIDCross sectionID × CS, mmOD
    -2010.171 ± 0.005"0.139 ± 0.004"4.34 × 3.530.449"
    -2020.234 ± 0.005"0.139 ± 0.004"5.94 × 3.530.512"
    -2030.296 ± 0.005"0.139 ± 0.004"7.52 × 3.530.574"
    -2040.359 ± 0.005"0.139 ± 0.004"9.12 × 3.530.637"
    -2050.421 ± 0.005"0.139 ± 0.004"10.69 × 3.530.699"
    -2060.484 ± 0.005"0.139 ± 0.004"12.29 × 3.530.762"
    -2070.546 ± 0.007"0.139 ± 0.004"13.87 × 3.530.824"
    -2080.609 ± 0.009"0.139 ± 0.004"15.47 × 3.530.887"
    -2090.671 ± 0.009"0.139 ± 0.004"17.04 × 3.530.949"
    -2100.734 ± 0.010"0.139 ± 0.004"18.64 × 3.531.012"
    -2110.796 ± 0.010"0.139 ± 0.004"20.22 × 3.531.074"
    -2120.859 ± 0.010"0.139 ± 0.004"21.82 × 3.531.137"
    -2130.921 ± 0.010"0.139 ± 0.004"23.39 × 3.531.199"
    -2140.984 ± 0.010"0.139 ± 0.004"24.99 × 3.531.262"
    -2151.046 ± 0.010"0.139 ± 0.004"26.57 × 3.531.324"
    -2161.109 ± 0.012"0.139 ± 0.004"28.17 × 3.531.387"
    -2171.171 ± 0.012"0.139 ± 0.004"29.74 × 3.531.449"
    -2181.234 ± 0.012"0.139 ± 0.004"31.34 × 3.531.512"
    -2191.296 ± 0.012"0.139 ± 0.004"32.92 × 3.531.574"
    -2201.359 ± 0.012"0.139 ± 0.004"34.52 × 3.531.637"
    -2211.421 ± 0.012"0.139 ± 0.004"36.09 × 3.531.699"
    -2221.484 ± 0.015"0.139 ± 0.004"37.69 × 3.531.762"
    -2231.609 ± 0.015"0.139 ± 0.004"40.87 × 3.531.887"
    -2241.734 ± 0.015"0.139 ± 0.004"44.04 × 3.532.012"
    -2251.859 ± 0.018"0.139 ± 0.004"47.22 × 3.532.137"
    -2261.984 ± 0.018"0.139 ± 0.004"50.39 × 3.532.262"
    -2272.109 ± 0.018"0.139 ± 0.004"53.57 × 3.532.387"
    -2282.234 ± 0.020"0.139 ± 0.004"56.74 × 3.532.512"
    -2292.359 ± 0.020"0.139 ± 0.004"59.92 × 3.532.637"
    -2302.484 ± 0.020"0.139 ± 0.004"63.09 × 3.532.762"
    -2312.609 ± 0.020"0.139 ± 0.004"66.27 × 3.532.887"
    -2322.734 ± 0.024"0.139 ± 0.004"69.44 × 3.533.012"
    -2332.859 ± 0.024"0.139 ± 0.004"72.62 × 3.533.137"
    -2342.984 ± 0.024"0.139 ± 0.004"75.79 × 3.533.262"
    -2353.109 ± 0.024"0.139 ± 0.004"78.97 × 3.533.387"
    -2363.234 ± 0.024"0.139 ± 0.004"82.14 × 3.533.512"
    -2373.359 ± 0.024"0.139 ± 0.004"85.32 × 3.533.637"
    -2383.484 ± 0.024"0.139 ± 0.004"88.49 × 3.533.762"
    -2393.609 ± 0.028"0.139 ± 0.004"91.67 × 3.533.887"
    -2403.734 ± 0.028"0.139 ± 0.004"94.84 × 3.534.012"
    -2413.859 ± 0.028"0.139 ± 0.004"98.02 × 3.534.137"
    -2423.984 ± 0.028"0.139 ± 0.004"101.19 × 3.534.262"
    -2434.109 ± 0.028"0.139 ± 0.004"104.37 × 3.534.387"
    -2444.234 ± 0.030"0.139 ± 0.004"107.54 × 3.534.512"
    -2454.359 ± 0.030"0.139 ± 0.004"110.72 × 3.534.637"
    -2464.484 ± 0.030"0.139 ± 0.004"113.89 × 3.534.762"
    -2474.609 ± 0.030"0.139 ± 0.004"117.07 × 3.534.887"
    -2484.734 ± 0.030"0.139 ± 0.004"120.24 × 3.535.012"
    -2494.859 ± 0.035"0.139 ± 0.004"123.42 × 3.535.137"
    -2504.984 ± 0.035"0.139 ± 0.004"126.59 × 3.535.262"
    -2515.109 ± 0.035"0.139 ± 0.004"129.77 × 3.535.387"
    -2525.234 ± 0.035"0.139 ± 0.004"132.94 × 3.535.512"
    -2535.359 ± 0.035"0.139 ± 0.004"136.12 × 3.535.637"
    -2545.484 ± 0.035"0.139 ± 0.004"139.29 × 3.535.762"
    -2555.609 ± 0.035"0.139 ± 0.004"142.47 × 3.535.887"
    -2565.734 ± 0.035"0.139 ± 0.004"145.64 × 3.536.012"
    -2575.859 ± 0.035"0.139 ± 0.004"148.82 × 3.536.137"
    -2585.984 ± 0.035"0.139 ± 0.004"151.99 × 3.536.262"
    -2596.234 ± 0.040"0.139 ± 0.004"158.34 × 3.536.512"
    -2606.484 ± 0.040"0.139 ± 0.004"164.69 × 3.536.762"
    -2616.734 ± 0.040"0.139 ± 0.004"171.04 × 3.537.012"
    -2626.984 ± 0.040"0.139 ± 0.004"177.39 × 3.537.262"
    -2637.234 ± 0.045"0.139 ± 0.004"183.74 × 3.537.512"
    -2647.484 ± 0.045"0.139 ± 0.004"190.09 × 3.537.762"
    -2657.734 ± 0.045"0.139 ± 0.004"196.44 × 3.538.012"
    -2667.984 ± 0.045"0.139 ± 0.004"202.79 × 3.538.262"
    -2678.234 ± 0.050"0.139 ± 0.004"209.14 × 3.538.512"
    -2688.484 ± 0.050"0.139 ± 0.004"215.49 × 3.538.762"
    -2698.734 ± 0.050"0.139 ± 0.004"221.84 × 3.539.012"
    -2708.984 ± 0.050"0.139 ± 0.004"228.19 × 3.539.262"
    -2719.234 ± 0.055"0.139 ± 0.004"234.54 × 3.539.512"
    -2729.484 ± 0.055"0.139 ± 0.004"240.89 × 3.539.762"
    -2739.734 ± 0.055"0.139 ± 0.004"247.24 × 3.5310.012"
    -2749.984 ± 0.055"0.139 ± 0.004"253.59 × 3.5310.262"
    -27510.484 ± 0.055"0.139 ± 0.004"266.29 × 3.5310.762"
    -27610.984 ± 0.065"0.139 ± 0.004"278.99 × 3.5311.262"
    -27711.484 ± 0.065"0.139 ± 0.004"291.69 × 3.5311.762"
    -27811.984 ± 0.065"0.139 ± 0.004"304.39 × 3.5312.262"
    -27912.984 ± 0.065"0.139 ± 0.004"329.79 × 3.5313.262"
    -28013.984 ± 0.065"0.139 ± 0.004"355.19 × 3.5314.262"
    -28114.984 ± 0.065"0.139 ± 0.004"380.59 × 3.5315.262"
    -28215.955 ± 0.075"0.139 ± 0.004"405.26 × 3.5316.233"
    -28316.955 ± 0.080"0.139 ± 0.004"430.66 × 3.5317.233"
    -28417.955 ± 0.085"0.139 ± 0.004"456.06 × 3.5318.233"

    300 series

    AS568 300 series: inside diameter, cross section and outside diameter
    DashIDCross sectionID × CS, mmOD
    -3090.412 ± 0.005"0.210 ± 0.005"10.46 × 5.330.832"
    -3100.475 ± 0.005"0.210 ± 0.005"12.07 × 5.330.895"
    -3110.537 ± 0.007"0.210 ± 0.005"13.64 × 5.330.957"
    -3120.600 ± 0.009"0.210 ± 0.005"15.24 × 5.331.020"
    -3130.662 ± 0.009"0.210 ± 0.005"16.81 × 5.331.082"
    -3140.725 ± 0.010"0.210 ± 0.005"18.42 × 5.331.145"
    -3150.787 ± 0.010"0.210 ± 0.005"19.99 × 5.331.207"
    -3160.850 ± 0.010"0.210 ± 0.005"21.59 × 5.331.270"
    -3170.912 ± 0.010"0.210 ± 0.005"23.16 × 5.331.332"
    -3180.975 ± 0.010"0.210 ± 0.005"24.77 × 5.331.395"
    -3191.037 ± 0.010"0.210 ± 0.005"26.34 × 5.331.457"
    -3201.100 ± 0.012"0.210 ± 0.005"27.94 × 5.331.520"
    -3211.162 ± 0.012"0.210 ± 0.005"29.51 × 5.331.582"
    -3221.225 ± 0.012"0.210 ± 0.005"31.12 × 5.331.645"
    -3231.287 ± 0.012"0.210 ± 0.005"32.69 × 5.331.707"
    -3241.350 ± 0.012"0.210 ± 0.005"34.29 × 5.331.770"
    -3251.475 ± 0.015"0.210 ± 0.005"37.47 × 5.331.895"
    -3261.600 ± 0.015"0.210 ± 0.005"40.64 × 5.332.020"
    -3271.725 ± 0.015"0.210 ± 0.005"43.82 × 5.332.145"
    -3281.850 ± 0.015"0.210 ± 0.005"46.99 × 5.332.270"
    -3291.975 ± 0.018"0.210 ± 0.005"50.17 × 5.332.395"
    -3302.100 ± 0.018"0.210 ± 0.005"53.34 × 5.332.520"
    -3312.225 ± 0.018"0.210 ± 0.005"56.52 × 5.332.645"
    -3322.350 ± 0.018"0.210 ± 0.005"59.69 × 5.332.770"
    -3332.475 ± 0.020"0.210 ± 0.005"62.87 × 5.332.895"
    -3342.600 ± 0.020"0.210 ± 0.005"66.04 × 5.333.020"
    -3352.725 ± 0.020"0.210 ± 0.005"69.22 × 5.333.145"
    -3362.850 ± 0.020"0.210 ± 0.005"72.39 × 5.333.270"
    -3372.975 ± 0.024"0.210 ± 0.005"75.57 × 5.333.395"
    -3383.100 ± 0.024"0.210 ± 0.005"78.74 × 5.333.520"
    -3393.225 ± 0.024"0.210 ± 0.005"81.92 × 5.333.645"
    -3403.350 ± 0.024"0.210 ± 0.005"85.09 × 5.333.770"
    -3413.475 ± 0.024"0.210 ± 0.005"88.27 × 5.333.895"
    -3423.600 ± 0.028"0.210 ± 0.005"91.44 × 5.334.020"
    -3433.725 ± 0.028"0.210 ± 0.005"94.62 × 5.334.145"
    -3443.850 ± 0.028"0.210 ± 0.005"97.79 × 5.334.270"
    -3453.975 ± 0.028"0.210 ± 0.005"100.97 × 5.334.395"
    -3464.100 ± 0.028"0.210 ± 0.005"104.14 × 5.334.520"
    -3474.225 ± 0.030"0.210 ± 0.005"107.32 × 5.334.645"
    -3484.350 ± 0.030"0.210 ± 0.005"110.49 × 5.334.770"
    -3494.475 ± 0.030"0.210 ± 0.005"113.67 × 5.334.895"
    -3504.600 ± 0.030"0.210 ± 0.005"116.84 × 5.335.020"
    -3514.725 ± 0.030"0.210 ± 0.005"120.02 × 5.335.145"
    -3524.850 ± 0.030"0.210 ± 0.005"123.19 × 5.335.270"
    -3534.975 ± 0.037"0.210 ± 0.005"126.37 × 5.335.395"
    -3545.100 ± 0.037"0.210 ± 0.005"129.54 × 5.335.520"
    -3555.225 ± 0.037"0.210 ± 0.005"132.72 × 5.335.645"
    -3565.350 ± 0.037"0.210 ± 0.005"135.89 × 5.335.770"
    -3575.475 ± 0.037"0.210 ± 0.005"139.07 × 5.335.895"
    -3585.600 ± 0.037"0.210 ± 0.005"142.24 × 5.336.020"
    -3595.725 ± 0.037"0.210 ± 0.005"145.42 × 5.336.145"
    -3605.850 ± 0.037"0.210 ± 0.005"148.59 × 5.336.270"
    -3615.975 ± 0.037"0.210 ± 0.005"151.77 × 5.336.395"
    -3626.225 ± 0.040"0.210 ± 0.005"158.12 × 5.336.645"
    -3636.475 ± 0.040"0.210 ± 0.005"164.47 × 5.336.895"
    -3646.725 ± 0.040"0.210 ± 0.005"170.82 × 5.337.145"
    -3656.975 ± 0.040"0.210 ± 0.005"177.17 × 5.337.395"
    -3667.225 ± 0.045"0.210 ± 0.005"183.52 × 5.337.645"
    -3677.475 ± 0.045"0.210 ± 0.005"189.87 × 5.337.895"
    -3687.725 ± 0.045"0.210 ± 0.005"196.22 × 5.338.145"
    -3697.975 ± 0.045"0.210 ± 0.005"202.57 × 5.338.395"
    -3708.225 ± 0.050"0.210 ± 0.005"208.92 × 5.338.645"
    -3718.475 ± 0.050"0.210 ± 0.005"215.27 × 5.338.895"
    -3728.725 ± 0.050"0.210 ± 0.005"221.62 × 5.339.145"
    -3738.975 ± 0.050"0.210 ± 0.005"227.97 × 5.339.395"
    -3749.225 ± 0.055"0.210 ± 0.005"234.32 × 5.339.645"
    -3759.475 ± 0.055"0.210 ± 0.005"240.67 × 5.339.895"
    -3769.725 ± 0.055"0.210 ± 0.005"247.02 × 5.3310.145"
    -3779.975 ± 0.055"0.210 ± 0.005"253.37 × 5.3310.395"
    -37810.475 ± 0.060"0.210 ± 0.005"266.07 × 5.3310.895"
    -37910.975 ± 0.060"0.210 ± 0.005"278.77 × 5.3311.395"
    -38011.475 ± 0.065"0.210 ± 0.005"291.47 × 5.3311.895"
    -38111.975 ± 0.065"0.210 ± 0.005"304.17 × 5.3312.395"
    -38212.975 ± 0.065"0.210 ± 0.005"329.57 × 5.3313.395"
    -38313.975 ± 0.070"0.210 ± 0.005"354.97 × 5.3314.395"
    -38414.975 ± 0.070"0.210 ± 0.005"380.37 × 5.3315.395"
    -38515.955 ± 0.075"0.210 ± 0.005"405.26 × 5.3316.375"
    -38616.955 ± 0.080"0.210 ± 0.005"430.66 × 5.3317.375"
    -38717.955 ± 0.085"0.210 ± 0.005"456.06 × 5.3318.375"
    -38818.955 ± 0.090"0.210 ± 0.005"481.46 × 5.3319.375"
    -38919.955 ± 0.095"0.210 ± 0.005"506.86 × 5.3320.375"
    -39020.955 ± 0.095"0.210 ± 0.005"532.26 × 5.3321.375"
    -39121.995 ± 0.100" or 21.955 ± 0.100"

    Two charts disagree: Greene Tweed 21.995 ± 0.100", Freudenberg-Simrit 21.955 ± 0.100"

    0.210 ± 0.005"——
    -39222.940 ± 0.105"0.210 ± 0.005"582.68 × 5.3323.360"
    -39323.940 ± 0.110"0.210 ± 0.005"608.08 × 5.3324.360"
    -39424.940 ± 0.115"0.210 ± 0.005"633.48 × 5.3325.360"
    -39525.940 ± 0.120"0.210 ± 0.005"658.88 × 5.3326.360"

    400 series

    AS568 400 series: inside diameter, cross section and outside diameter
    DashIDCross sectionID × CS, mmOD
    -4254.475 ± 0.033"0.275 ± 0.006"113.67 × 6.995.025"
    -4264.600 ± 0.033"0.275 ± 0.006"116.84 × 6.995.150"
    -4274.725 ± 0.033"0.275 ± 0.006"120.02 × 6.995.275"
    -4284.850 ± 0.033"0.275 ± 0.006"123.19 × 6.995.400"
    -4294.975 ± 0.037"0.275 ± 0.006"126.37 × 6.995.525"
    -4305.100 ± 0.037"0.275 ± 0.006"129.54 × 6.995.650"
    -4315.225 ± 0.037"0.275 ± 0.006"132.72 × 6.995.775"
    -4325.350 ± 0.037"0.275 ± 0.006"135.89 × 6.995.900"
    -4335.475 ± 0.037"0.275 ± 0.006"139.07 × 6.996.025"
    -4345.600 ± 0.037"0.275 ± 0.006"142.24 × 6.996.150"
    -4355.725 ± 0.037"0.275 ± 0.006"145.42 × 6.996.275"
    -4365.850 ± 0.037"0.275 ± 0.006"148.59 × 6.996.400"
    -4375.975 ± 0.037"0.275 ± 0.006"151.77 × 6.996.525"
    -4386.225 ± 0.040"0.275 ± 0.006"158.12 × 6.996.775"
    -4396.475 ± 0.040"0.275 ± 0.006"164.47 × 6.997.025"
    -4406.725 ± 0.040"0.275 ± 0.006"170.82 × 6.997.275"
    -4416.975 ± 0.040"0.275 ± 0.006"177.17 × 6.997.525"
    -4427.225 ± 0.045"0.275 ± 0.006"183.52 × 6.997.775"
    -4437.475 ± 0.045"0.275 ± 0.006"189.87 × 6.998.025"
    -4447.725 ± 0.045"0.275 ± 0.006"196.22 × 6.998.275"
    -4457.975 ± 0.045"0.275 ± 0.006"202.57 × 6.998.525"
    -4468.475 ± 0.055"0.275 ± 0.006"215.27 × 6.999.025"
    -4478.975 ± 0.055"0.275 ± 0.006"227.97 × 6.999.525"
    -4489.475 ± 0.055"0.275 ± 0.006"240.67 × 6.9910.025"
    -4499.975 ± 0.055"0.275 ± 0.006"253.37 × 6.9910.525"
    -45010.475 ± 0.060"0.275 ± 0.006"266.07 × 6.9911.025"
    -45110.975 ± 0.060"0.275 ± 0.006"278.77 × 6.9911.525"
    -45211.475 ± 0.060"0.275 ± 0.006"291.47 × 6.9912.025"
    -45311.975 ± 0.060"0.275 ± 0.006"304.17 × 6.9912.525"
    -45412.475 ± 0.060"0.275 ± 0.006"316.87 × 6.9913.025"
    -45512.975 ± 0.060"0.275 ± 0.006"329.57 × 6.9913.525"
    -45613.475 ± 0.070"0.275 ± 0.006"342.27 × 6.9914.025"
    -45713.975 ± 0.070"0.275 ± 0.006"354.97 × 6.9914.525"
    -45814.475 ± 0.070"0.275 ± 0.006"367.67 × 6.9915.025"
    -45914.975 ± 0.070"0.275 ± 0.006"380.37 × 6.9915.525"
    -46015.475 ± 0.070"0.275 ± 0.006"393.07 × 6.9916.025"
    -46115.955 ± 0.075"0.275 ± 0.006"405.26 × 6.9916.505"
    -46216.455 ± 0.075"0.275 ± 0.006"417.96 × 6.9917.005"
    -46316.955 ± 0.080"0.275 ± 0.006"430.66 × 6.9917.505"
    -46417.455 ± 0.085"0.275 ± 0.006"443.36 × 6.9918.005"
    -46517.955 ± 0.085"0.275 ± 0.006"456.06 × 6.9918.505"
    -46618.455 ± 0.085"0.275 ± 0.006"468.76 × 6.9919.005"
    -46718.955 ± 0.090"0.275 ± 0.006"481.46 × 6.9919.505"
    -46819.455 ± 0.090"0.275 ± 0.006"494.16 × 6.9920.005"
    -46919.955 ± 0.095"0.275 ± 0.006"506.86 × 6.9920.505"
    -47020.955 ± 0.095"0.275 ± 0.006"532.26 × 6.9921.505"
    -47121.955 ± 0.100"0.275 ± 0.006"557.66 × 6.9922.505"
    -47222.940 ± 0.105"0.275 ± 0.006"582.68 × 6.9923.490"
    -47323.940 ± 0.110"0.275 ± 0.006"608.08 × 6.9924.490"
    -47424.940 ± 0.115"0.275 ± 0.006"633.48 × 6.9925.490"
    -47525.940 ± 0.120"0.275 ± 0.006"658.88 × 6.9926.490"
    Sources3

    Every ID and cross section is checked against two or three published copies of AS568, unless a tag says otherwise. Millimetres are the inch values × 25.4, and OD is ID + 2 × CS.