AS568-102 is 0.049 ± 0.005" or 0.049 ± 0.004" ID × 0.103 ± 0.003" cross section, the copies differing on the ID. For a static radial seal, cut the groove 0.080–0.086" deep and 0.140–0.151" wide (Parker and Apple Rubber).

A 0.103" O-ring cross section in a static radial gland, in section: squeezed between the groove bottom and the bore, its free section dashed over it.free section 0.103"squeeze 14–25 %boreO-ringgland depth 0.080–0.086"gland width 0.140–0.151"piston
AS568-102 in a static radial gland. Drawn to scale at the gland’s middle depth and width.

Size and tolerances

Inside diameter
0.049 ± 0.005" or 0.049 ± 0.004"
Cross section
0.103 ± 0.003" (2.62 mm)
Outside diameter
Not given: the copies differ on the size

Two charts disagree: Freudenberg-Simrit and Global O-Ring 0.049 ± 0.005", Greene Tweed 0.049 ± 0.004"

AS568 sizes are nominal inch sizes; the tolerances are the ones the copies print. The first digit of the dash number is the cross-section series, so every 100 series ring shares this cross section.

Groove for a 0.103" cross section

Depth and width as a range spanning Parker’s and Apple Rubber’s gland tables. For the bore and gland diameters, use the groove calculator.

Gland depth and width for AS568-102, by seal type
SealDepthWidth
Static radial (piston or rod)0.080–0.086"0.140–0.151"
Face seal0.074–0.081"0.136–0.151"
Dynamic (reciprocating)0.087–0.090"0.140–0.150"

Only two makers publish this: Parker and Apple Rubber