AS568 · 200 series

AS568-248 O-ring size

AS568-248 is 4.734" ID × 0.139" cross section (120.24 × 3.53 mm), held to ± 0.030" and ± 0.004", 5.012" OD, checked against 3 published copies. For a static radial seal, cut the groove 0.110–0.116" deep and 0.187–0.200" wide (Parker and Apple Rubber).

A 0.139" O-ring cross section in a static radial gland, in section: squeezed between the groove bottom and the bore, its free section dashed over it.free section 0.139"squeeze 14–23 %boreO-ringgland depth 0.110–0.116"gland width 0.187–0.200"piston
AS568-248 in a static radial gland. Drawn to scale at the gland’s middle depth and width.

Size and tolerances

Inside diameter
4.734 ± 0.030" (120.24 mm)
Cross section
0.139 ± 0.004" (3.53 mm)
Outside diameter
5.012" (ID + 2 × cross section)

Two published copies agree

AS568 sizes are nominal inch sizes; the tolerances are the ones the copies print. The first digit of the dash number is the cross-section series, so every 200 series ring shares this cross section.

Groove for a 0.139" cross section

Depth and width as a range spanning Parker’s and Apple Rubber’s gland tables. For the bore and gland diameters, use the groove calculator.

Gland depth and width for AS568-248, by seal type
SealDepthWidth
Static radial (piston or rod)0.110–0.116"0.187–0.200"
Face seal0.100–0.108"0.177–0.200"
Dynamic (reciprocating)0.119–0.123"0.180–0.192"

Only two makers publish this: Parker and Apple Rubber