AS568 · 300 series
AS568-315 O-ring size
AS568-315 is 0.787" ID × 0.210" cross section (19.99 × 5.33 mm), held to ± 0.010" and ± 0.005", 1.207" OD, checked against 3 published copies. For a static radial seal, cut the groove 0.170–0.176" deep and 0.275–0.286" wide (Parker and Apple Rubber).
Size and tolerances
- Inside diameter
- 0.787 ± 0.010" (19.99 mm)
- Cross section
- 0.210 ± 0.005" (5.33 mm)
- Outside diameter
- 1.207" (ID + 2 × cross section)
Two published copies agree
AS568 sizes are nominal inch sizes; the tolerances are the ones the copies print. The first digit of the dash number is the cross-section series, so every 300 series ring shares this cross section.
Groove for a 0.210" cross section
Depth and width as a range spanning Parker’s and Apple Rubber’s gland tables. For the bore and gland diameters, use the groove calculator.
| Seal | Depth | Width |
|---|---|---|
| Static radial (piston or rod) | 0.170–0.176" | 0.275–0.286" |
| Face seal | 0.152–0.165" | 0.270–0.290" |
| Dynamic (reciprocating) | 0.183–0.188" | 0.280–0.290" |
Only two makers publish this: Parker and Apple Rubber
Other sizes
Sources
Sources5
The size is checked against published copies of AS568; the groove spans two makers’ gland tables.
- Greene Tweed, AS568 standard O-ring sizing (archived Jun 9, 2026)
- Freudenberg-Simrit, AS568 O-ring sizes (via All Seals) (archived Feb 7, 2025)
- Global O-Ring and Seal, AS568 guide (archived Sep 14, 2025)
- Parker O-Ring Handbook ORD 5700: Design Charts 4-2, 4-3 and 5-2 (archived Dec 27, 2025)
- Apple Rubber, Seal Design Guide Table A: gland design for static and dynamic seals (archived Mar 26, 2024)