AS568 · 400 series

AS568-436 O-ring size

AS568-436 is 5.850" ID × 0.275" cross section (148.59 × 6.99 mm), held to ± 0.037" and ± 0.006", 6.400" OD, checked against 3 published copies. For a static radial seal, cut the groove 0.225–0.235" deep and 0.345–0.380" wide (Parker and Apple Rubber).

A 0.275" O-ring cross section in a static radial gland, in section: squeezed between the groove bottom and the bore, its free section dashed over it.free section 0.275"squeeze 13–20 %boreO-ringgland depth 0.225–0.235"gland width 0.345–0.380"piston
AS568-436 in a static radial gland. Drawn to scale at the gland’s middle depth and width.

Size and tolerances

Inside diameter
5.850 ± 0.037" (148.59 mm)
Cross section
0.275 ± 0.006" (6.99 mm)
Outside diameter
6.400" (ID + 2 × cross section)

Two published copies agree

AS568 sizes are nominal inch sizes; the tolerances are the ones the copies print. The first digit of the dash number is the cross-section series, so every 400 series ring shares this cross section.

Groove for a 0.275" cross section

Depth and width as a range spanning Parker’s and Apple Rubber’s gland tables. For the bore and gland diameters, use the groove calculator.

Gland depth and width for AS568-436, by seal type
SealDepthWidth
Static radial (piston or rod)0.225–0.235"0.345–0.380"
Face seal0.201–0.215"0.342–0.362"
Dynamic (reciprocating)0.234–0.240"0.370–0.380"

Only two makers publish this: Parker and Apple Rubber

O-ring groove calculator · O-ring groove chart

Other sizes

Sources

Sources5