Pipe schedule chart

1/2" pipe schedule

NPS 1/2 (DN 15) pipe is 0.840" outside diameter in every schedule. Schedule 40 has a 0.109" wall and a 0.622" ID; Schedule 80 has a 0.147" wall and a 0.546" ID. The schedule sets the wall: ID = OD − 2 × wall.

The pipe's cross section, 0.84" OD, in Schedule 40 and Schedule 80: the same OD, the wall setting the bore.OD 0.84"schedule 40ID 0.622"wall 0.109"schedule 80ID 0.546"wall 0.147"
0.84" OD pipe in Schedule 40 and Schedule 80. Each ring drawn to scale; the two to the same scale.

Outside diameter

0.840"21.34 mm

NPS 1/2 · DN 15

Checked against 5 published copies

Units

Every schedule

Thinnest wall first. Schedules that share a wall share a row. Weight is plain-end carbon steel.

1/2" pipe wall, inside diameter, weight and areas by schedule
ScheduleWall (in)(mm)ID (in)(mm)Weight (lb/ft)(kg/m)Metal area (in²)(cm²)Flow area (in²)(cm²)Checked
5S0.0651.650.71018.030.540.800.1581.020.3962.55Checked against 4 published copies
Sch 10 · 10S0.0832.110.67417.120.671.000.1971.270.3572.30Checked against 3 published copies
STD · Sch 40 · 40S0.1092.770.62215.800.851.270.2501.610.3041.96Checked against 3 published copies
XS · Sch 80 · 80S0.1473.730.54613.871.091.620.3202.060.2341.51Checked against 4 published copies
Sch 1600.1884.780.46411.791.311.950.3852.480.1691.09Checked against 4 published copies
XXS0.2947.470.2526.401.722.550.5043.250.0500.32Checked against 4 published copies

Checked against 3 published copies

  • STD: Guanyu Tube (TubingChina) prints 0.119"; the other copies print 0.109".
  • Sch 40: Guanyu Tube (TubingChina) prints 0.119"; the other copies print 0.109".
  • 40S: Guanyu Tube (TubingChina) prints 0.119"; the other copies print 0.109".

Notes for 1/2" pipe

STD and XS, stainless, weight and what's not shown
  • STD and Sch 40 are the same wall here (0.109"). They part above NPS 10.
  • XS and Sch 80 are the same wall here (0.147"). They part above NPS 8.
  • Schedules ending in S are stainless (ASME B36.19M). Same OD; the wall can differ from the carbon schedule of the same number.
  • The weight is B36.10M's plain-end formula for carbon steel, 10.69 × (OD − wall) × wall lb/ft. For stainless or another metal, use the metal weight calculator (round tube, OD 0.840").