Pipe schedule chart

Every pipe of one nominal size (NPS) has the same outside diameter; the schedule sets the wall, so a heavier schedule has a smaller bore. 2" pipe is 2.375" OD in every schedule, with a 0.154" wall in Sch 40. Carbon and alloy steel follow ASME B36.10M; stainless follows B36.19M, whose schedules end in S.

Printable pipe schedule chart (one page)NPT pipe threads and tap drillsMetal weight calculator

Units

Carbon and alloy steel: wall thickness (ASME B36.10M)

Inches.Millimetres, converted from the inch values. Tap a size for its ID, weight per foot and areas. A dash means the standard lists no such wall, or fewer than two published copies print it.

Carbon and alloy steel pipe outside diameter and wall thickness by NPS and schedule
NPSDNODSch 10Sch 20Sch 30STDSch 40Sch 60XSSch 80Sch 100Sch 120Sch 140Sch 160XXS
1/8"60.40510.290.0491.24——0.0681.730.0681.73—0.0952.410.0952.41—————
1/4"80.54013.720.0651.65——0.0882.240.0882.24—0.1193.020.1193.02—————
3/8"100.67517.150.0651.65——0.0912.310.0912.31—0.1263.200.1263.20—————
1/2"150.84021.340.0832.11——0.1092.770.1092.77—0.1473.730.1473.73———0.1884.780.2947.47
3/4"201.05026.670.0832.11——0.1132.870.1132.87—0.1543.910.1543.91———0.2195.560.3087.82
1"251.31533.400.1092.77——0.1333.380.1333.38—0.1794.550.1794.55———0.2506.350.3589.09
1-1/4"321.66042.160.1092.77——0.1403.560.1403.56—0.1914.850.1914.85———0.2506.350.3829.70
1-1/2"401.90048.260.1092.77——0.1453.680.1453.68—0.2005.080.2005.08———0.2817.140.40010.16
2"502.37560.330.1092.77——0.1543.910.1543.91—0.2185.540.2185.54———0.3448.740.43611.07
2-1/2"652.87573.030.1203.05——0.2035.160.2035.16—0.2767.010.2767.01———0.3759.530.55214.02
3"803.50088.900.1203.05——0.2165.490.2165.49—0.3007.620.3007.62———0.43811.130.60015.24
3-1/2"904.000101.600.1203.05——0.2265.740.2265.74—0.3188.080.3188.08————0.63616.15
4"1004.500114.300.1203.05——0.2376.020.2376.02—0.3378.560.3378.56—0.43811.13—0.53113.490.67417.12
5"1255.563141.300.1343.40——0.2586.550.2586.55—0.3759.530.3759.53—0.50012.70—0.62515.880.75019.05
6"1506.625168.280.1343.40——0.2807.110.2807.11—0.43210.970.43210.97—0.56214.27—0.71918.260.86421.95
8"2008.625219.080.1483.760.2506.350.2777.040.3228.180.3228.180.40610.310.50012.700.50012.700.59415.090.71918.260.81220.620.90623.010.87522.23
10"25010.750273.050.1654.190.2506.350.3077.800.3659.270.3659.270.50012.700.50012.700.59415.090.71918.260.84421.441.00025.401.12528.58—
12"30012.750323.850.1804.570.2506.350.3308.380.3759.530.40610.310.56214.270.50012.700.68817.480.84421.441.00025.401.12528.581.31233.32—
14"35014.000355.600.2506.350.3127.920.3759.530.3759.530.43811.130.59415.090.50012.700.75019.050.93823.831.09427.791.25031.751.40635.71—
16"40016.000406.400.2506.350.3127.920.3759.530.3759.530.50012.700.65616.660.50012.700.84421.441.03126.191.21930.961.43836.531.59440.49—
18"45018.000457.200.2506.350.3127.920.43811.130.3759.530.56214.270.75019.050.50012.700.93823.831.15629.361.37534.931.56239.671.78145.24—
20"50020.000508.000.2506.350.3759.530.50012.700.3759.530.59415.090.81220.620.50012.701.03126.191.28132.541.50038.101.75044.451.96950.01—
22"55022.000558.800.2506.350.3759.530.50012.700.3759.53—0.87522.230.50012.701.12528.581.37534.931.62541.281.87547.632.12553.98—
24"60024.000609.600.2506.350.3759.530.56214.270.3759.530.68817.480.96924.610.50012.701.21930.961.53138.891.81246.022.06252.372.34459.54—
26"65026.000660.400.3127.920.50012.70—0.3759.53——0.50012.70——————
28"70028.000711.200.3127.920.50012.700.62515.880.3759.53——0.50012.70——————
30"75030.000762.000.3127.920.50012.700.62515.880.3759.53——0.50012.70——————
32"80032.000812.800.3127.920.50012.700.62515.880.3759.530.68817.48—0.50012.70——————
34"85034.000863.600.3127.920.50012.700.62515.880.3759.530.68817.48—0.50012.70——————
36"90036.000914.400.3127.92—0.62515.880.3759.530.75019.05—0.50012.70——————

Stainless steel: wall thickness (ASME B36.19M)

Same ODs as carbon pipe. B36.19M runs to NPS 30, and lists 40S and 80S only to NPS 24.

Stainless steel pipe outside diameter and wall thickness by NPS and schedule
NPSOD5S10S40S80S
1/8"0.40510.29—0.0491.240.0681.730.0952.41
1/4"0.54013.72—0.0651.650.0882.240.1193.02
3/8"0.67517.15—0.0651.650.0912.310.1263.20
1/2"0.84021.340.0651.650.0832.110.1092.770.1473.73
3/4"1.05026.670.0651.650.0832.110.1132.870.1543.91
1"1.31533.400.0651.650.1092.770.1333.380.1794.55
1-1/4"1.66042.160.0651.650.1092.770.1403.560.1914.85
1-1/2"1.90048.260.0651.650.1092.770.1453.680.2005.08
2"2.37560.330.0651.650.1092.770.1543.910.2185.54
2-1/2"2.87573.030.0832.110.1203.050.2035.160.2767.01
3"3.50088.900.0832.110.1203.050.2165.490.3007.62
3-1/2"4.000101.600.0832.110.1203.050.2265.740.3188.08
4"4.500114.300.0832.110.1203.050.2376.020.3378.56
5"5.563141.300.1092.770.1343.400.2586.550.3759.53
6"6.625168.280.1092.770.1343.400.2807.110.43210.97
8"8.625219.080.1092.770.1483.760.3228.180.50012.70
10"10.750273.050.1343.400.1654.190.3659.270.50012.70
12"12.750323.850.1563.960.1804.570.3759.530.50012.70
14"14.000355.600.1563.960.1884.780.3759.530.50012.70
16"16.000406.400.1654.190.1884.780.3759.530.50012.70
18"18.000457.200.1654.190.1884.780.3759.530.50012.70
20"20.000508.000.1884.780.2185.540.3759.530.50012.70
22"22.000558.80—0.218" or 0.25" (published copies disagree)——
24"24.000609.600.2185.540.2506.350.3759.530.50012.70
26"26.000660.40————
28"28.000711.20————
30"30.000762.000.2506.350.3127.92——

Schedule 40 and 80: ID and weight

Plain-end weight for carbon steel from B36.10M's formula, 10.69 × (OD − wall) × walllb/ft(shown in kg/m).

Schedule 40 and 80 pipe wall, inside diameter and weight per length by NPS
NPSSch 40Sch 80
WallIDlb/ftkg/mWallIDlb/ftkg/m
1/8"0.0681.730.2696.830.240.360.0952.410.2155.460.310.47
1/4"0.0882.240.3649.250.430.630.1193.020.3027.670.540.80
3/8"0.0912.310.49312.520.570.850.1263.200.42310.740.741.10
1/2"0.1092.770.62215.800.851.270.1473.730.54613.871.091.62
3/4"0.1132.870.82420.931.131.680.1543.910.74218.851.482.20
1"0.1333.381.04926.641.682.500.1794.550.95724.312.173.23
1-1/4"0.1403.561.38035.052.273.390.1914.851.27832.463.004.46
1-1/2"0.1453.681.61040.892.724.050.2005.081.50038.103.635.41
2"0.1543.912.06752.503.665.440.2185.541.93949.255.037.48
2-1/2"0.2035.162.46962.715.808.630.2767.012.32359.007.6711.41
3"0.2165.493.06877.937.5811.280.3007.622.90073.6610.2615.27
3-1/2"0.2265.743.54890.129.1213.570.3188.083.36485.4512.5218.63
4"0.2376.024.026102.2610.8016.070.3378.563.82697.1815.0022.32
5"0.2586.555.047128.1914.6321.770.3759.534.813122.2520.8030.95
6"0.2807.116.065154.0518.9928.260.43210.975.761146.3328.6042.56
8"0.3228.187.981202.7228.5842.530.50012.707.625193.6843.4364.63
10"0.3659.2710.020254.5140.5260.300.59415.099.562242.8764.4995.97
12"0.40610.3111.938303.2353.5779.730.68817.4811.374288.9088.71132.02
14"0.43811.1313.124333.3563.5094.500.75019.0512.500317.50106.23158.09
16"0.50012.7015.000381.0082.85123.290.84421.4414.312363.52136.74203.50
18"0.56214.2716.876428.65104.76155.910.93823.8316.124409.55171.08254.60
20"0.59415.0918.812477.82123.23183.381.03126.1917.938455.63209.06311.12
22"———1.12528.5819.750501.65251.05373.60
24"0.68817.4822.624574.65171.45255.151.21930.9621.562547.67296.86441.78
32"0.68817.4830.624777.85230.29342.71———
34"0.68817.4832.624828.65245.00364.60———
36"0.75019.0534.500876.30282.62420.58———

Reading a pipe schedule

Show
  • STD is Sch 40 up to NPS 10. Above that STD stays 0.375" while Sch 40 keeps growing (12": STD 0.375", Sch 40 0.406").
  • XS is Sch 80 up to NPS 8. Above that XS stays 0.500" (10": XS 0.500", Sch 80 0.594").
  • The S suffix means stainless (B36.19M). 40S and 80S match STD and XS; 10S matches Sch 10 up to NPS 12, then is thinner (14": 10S 0.188", Sch 10 0.250").
  • NPS is a name, not a size up to NPS 12: 2" pipe is 2.375" OD. From NPS 14 up the OD equals the NPS.
  • DN is the metric name for the same pipe (NPS 2 = DN 50); the pipe is the same.
  • XXS is not always the heaviest: at NPS 8, XXS is 0.875" and Sch 160 is 0.906".

Where each number comes from

Show

ASME B36.10M and B36.19M are the authority. Each wall is checked against 6 published copies of their tables, not averaged: a wall is shown when two or more agree. Copies that print a fraction cut off (0.593") instead of rounded (0.594") agree. NPS 2 Sch 40, for one:

Checked against 5 published copies

Copies that print something else

  • 1/2" Sch 40: Guanyu Tube (TubingChina) prints 0.119"; the others print 0.109".
  • 1/2" STD: Guanyu Tube (TubingChina) prints 0.119"; the others print 0.109".
  • 1/2" 40S: Guanyu Tube (TubingChina) prints 0.119"; the others print 0.109".
  • 4" Sch 160: Project Materials prints 0.674"; the others print 0.531".
  • 5" Sch 160: Project Materials prints 0.750"; the others print 0.625".
  • 12" 5S: Guanyu Tube (TubingChina) prints 0.165"; the others print 0.156".
  • 20" Sch 40: Guanyu Tube (TubingChina) prints 5.94"; the others print 0.594".
  • 20" Sch 60: Guanyu Tube (TubingChina) prints 8.12"; the others print 0.812".
  • 22" 10S: only two copies print it and they disagree, so both are shown.

Not shown

  • Printed by one copy only, so not shown until a second agrees:4" Sch 60 (Engineers Edge 0.281"), 4" Sch 140 (Project Materials 0.531"), 5" Sch 140 (Project Materials 0.625"), 6" Sch 100 (Project Materials 0.500"), 10" XXS (Project Materials 1.000"), 12" XXS (Project Materials 1.000").
  • 40S and 80S above NPS 24 and at NPS 22 (22", 26", 28", 30", 32", 34", 36"): some charts print them, but B36.19M lists none; those charts are relabelling STD and XS.

Weight

B36.10M's plain-end weight, W = 10.69 × (OD − wall) × wall lb/ft, for carbon steel. Most published charts still print weights from the 10.68 of older editions, about 0.1% lighter. Stainless is a little heavier: weigh it in the metal weight calculator as a round tube.

From the standard, ASME B36.10M (plain-end weight formula)

Sources11