Pipe schedule chart
1/8" pipe schedule
NPS 1/8 (DN 6) pipe is 0.405" outside diameter in every schedule. Schedule 40 has a 0.068" wall and a 0.269" ID; Schedule 80 has a 0.095" wall and a 0.215" ID. The schedule sets the wall: ID = OD − 2 × wall.
Outside diameter
0.405"10.29 mm
NPS 1/8 · DN 6
Checked against 5 published copies
Every schedule
Thinnest wall first. Schedules that share a wall share a row. Weight is plain-end carbon steel.
| Schedule | Wall (in)(mm) | ID (in)(mm) | Weight (lb/ft)(kg/m) | Metal area (in²)(cm²) | Flow area (in²)(cm²) | Checked |
|---|---|---|---|---|---|---|
| Sch 10 · 10S | 0.0491.24 | 0.3077.80 | 0.190.28 | 0.0550.35 | 0.0740.48 | Checked against 3 published copies |
| STD · Sch 40 · 40S | 0.0681.73 | 0.2696.83 | 0.240.36 | 0.0720.46 | 0.0570.37 | Checked against 4 published copies |
| XS · Sch 80 · 80S | 0.0952.41 | 0.2155.46 | 0.310.47 | 0.0930.60 | 0.0360.23 | Checked against 4 published copies |
Checked against 3 published copies
Notes for 1/8" pipe
STD and XS, stainless, weight and what's not shown
- STD and Sch 40 are the same wall here (0.068"). They part above NPS 10.
- XS and Sch 80 are the same wall here (0.095"). They part above NPS 8.
- Schedules ending in S are stainless (ASME B36.19M). Same OD; the wall can differ from the carbon schedule of the same number.
- The weight is B36.10M's plain-end formula for carbon steel, 10.69 × (OD − wall) × wall lb/ft. For stainless or another metal, use the metal weight calculator (round tube, OD 0.405").
Sources
Sources8
- ASME B36.10M, Welded and Seamless Wrought Steel Pipe (the authority for Sch 10–160, STD, XS, XXS)
- ASME B36.19M, Stainless Steel Pipe (the authority for 5S, 10S, 40S, 80S)
- Engineering ToolBox, ASME/ANSI B36.10/19 carbon, alloy and stainless steel pipe: dimensions (archived Oct 20, 2026)
- Engineers Edge, Standard pipe schedules and sizes chart (archived May 5, 2026)
- Project Materials, ASME B36.10 and B36.19 pipe sizes and schedules (inch, mm and lb/ft tables) (archived Jan 18, 2024)
- Guanyu Tube (TubingChina), ANSI standard steel pipe chart ASME B36.10 / B36.19 (archived Jun 30, 2025)
- Metal Supermarkets, Pipe schedule chart (Sch 40 and 80) (archived Apr 19, 2026)
- Project Materials, pipe weight: (OD − WT) × WT × 10.69 lb/ft for carbon steel (inch) (archived Jan 18, 2024)
Copies of B36.10M / B36.19M that print this size: Engineering ToolBox, Engineers Edge, Project Materials, Guanyu Tube (TubingChina), Metal Supermarkets.