Pipe schedule chart
28" pipe schedule
NPS 28 (DN 700) pipe is 28.000" outside diameter in every schedule. STD has a 0.375" wall and a 27.250" ID; XS has a 0.500" wall and a 27.000" ID. The schedule sets the wall: ID = OD − 2 × wall.
Outside diameter
28.000"711.20 mm
NPS 28 · DN 700
Checked against 4 published copies
Every schedule
Thinnest wall first. Schedules that share a wall share a row. Weight is plain-end carbon steel.
| Schedule | Wall (in)(mm) | ID (in)(mm) | Weight (lb/ft)(kg/m) | Metal area (in²)(cm²) | Flow area (in²)(cm²) | Checked |
|---|---|---|---|---|---|---|
| Sch 10 | 0.3127.92 | 27.376695.35 | 92.35137.43 | 27.139175.09 | 588.6133,797.50 | Checked against 3 published copies |
| STD | 0.3759.53 | 27.250692.15 | 110.74164.80 | 32.545209.97 | 583.2073,762.62 | Checked against 3 published copies |
| Sch 20 · XS | 0.50012.70 | 27.000685.80 | 146.99218.74 | 43.197278.69 | 572.5553,693.90 | Two published copies agree |
| Sch 30 | 0.62515.88 | 26.750679.45 | 182.90272.18 | 53.751346.78 | 562.0013,625.81 | Two published copies agree |
Two published copies agree
Notes for 28" pipe
STD and XS, stainless, weight and what's not shown
- Schedules ending in S are stainless (ASME B36.19M). Same OD; the wall can differ from the carbon schedule of the same number.
- The weight is B36.10M's plain-end formula for carbon steel, 10.69 × (OD − wall) × wall lb/ft. For stainless or another metal, use the metal weight calculator (round tube, OD 28.000").
- Not shown: 40S (B36.19M lists none at this size; Engineers Edge, Guanyu Tube (TubingChina) print STD/XS under it); 80S (B36.19M lists none at this size; Guanyu Tube (TubingChina) print STD/XS under it).
Sources
Sources9
- ASME B36.10M, Welded and Seamless Wrought Steel Pipe (the authority for Sch 10–160, STD, XS, XXS)
- ASME B36.19M, Stainless Steel Pipe (the authority for 5S, 10S, 40S, 80S)
- Wikipedia, Nominal Pipe Size: wall thickness tables (used only for the large-pipe cells no other copy prints; to be replaced) (archived Nov 9, 2026)
- Engineers Edge, Standard pipe schedules and sizes chart (archived May 5, 2026)
- Project Materials, ASME B36.10 and B36.19 pipe sizes and schedules (inch, mm and lb/ft tables) (archived Jan 18, 2024)
- Guanyu Tube (TubingChina), ANSI standard steel pipe chart ASME B36.10 / B36.19 (archived Jun 30, 2025)
- Project Materials, pipe weight: (OD − WT) × WT × 10.69 lb/ft for carbon steel (inch) (archived Jan 18, 2024)
- Project Materials, What is ASME B36.19? (scope NPS 1/8 to 30) (archived Apr 22, 2026)
- HT Pipe, ASME B36.19 (40S and 80S stop at NPS 24; 22 and 30 are 5S and 10S only) (archived Jul 12, 2026)
Copies of B36.10M / B36.19M that print this size: Wikipedia, Engineers Edge, Project Materials, Guanyu Tube (TubingChina).