Pipe schedule chart

34" pipe schedule

NPS 34 (DN 850) pipe is 34.000" outside diameter in every schedule. Schedule 40 has a 0.688" wall and a 32.624" ID; XS has a 0.500" wall and a 33.000" ID. The schedule sets the wall: ID = OD − 2 × wall.

The pipe's cross section, 34" OD, in Schedule 40 and XS: the same OD, the wall setting the bore.OD 34"schedule 40ID 32.624"wall 0.688"schedule XSID 33.000"wall 0.500"
34" OD pipe in Schedule 40 and XS. Each ring drawn to scale; the two to the same scale.

Outside diameter

34.000"863.60 mm

NPS 34 · DN 850

Checked against 4 published copies

Units

Every schedule

Thinnest wall first. Schedules that share a wall share a row. Weight is plain-end carbon steel.

34" pipe wall, inside diameter, weight and areas by schedule
ScheduleWall (in)(mm)ID (in)(mm)Weight (lb/ft)(kg/m)Metal area (in²)(cm²)Flow area (in²)(cm²)Checked
Sch 100.3127.9233.376847.75112.36167.2133.020213.03874.9005,644.51Checked against 3 published copies
STD0.3759.5333.250844.55134.79200.6039.614255.57868.3075,601.97Checked against 3 published copies
Sch 20 · XS0.50012.7033.000838.20179.06266.4752.622339.49855.2995,518.04Two published copies agree
Sch 300.62515.8832.750831.85222.99331.8465.532422.78842.3895,434.75Two published copies agree
Sch 400.68817.4832.624828.65245.00364.6072.001464.52835.9195,393.02Two published copies agree

Two published copies agree

Notes for 34" pipe

STD and XS, stainless, weight and what's not shown
  • STD (0.375") is not Sch 40 (0.688") at this size: they part above NPS 10.
  • B36.19M stainless schedules stop at NPS 30.
  • The weight is B36.10M's plain-end formula for carbon steel, 10.69 × (OD − wall) × wall lb/ft. For stainless or another metal, use the metal weight calculator (round tube, OD 34.000").
  • Not shown: 40S (B36.19M lists none at this size; Engineers Edge print STD/XS under it).

Sources

Sources8