Sheet metal gauge
6 gauge sheet metal thickness
6 gauge sheet metal is 0.1943" (4.93 mm) in steel and 0.1620" (4.12 mm) aluminum. Each metal has its own gauge system, and gauge is nominal: measure the stock when the thickness matters.
Steel
0.1943"
4.93 mm
Manufacturers' Standard Gauge
Aluminum
0.1620"
4.12 mm
Brown & Sharpe (AWG)
From the standard, Manufacturers' Standard Gauge
Weight
| Material | lb/ft² | kg/m² |
|---|---|---|
| Steel | 8.125 | 39.67 |
| Aluminum | 2.276 | 11.11 |
From the standard, Manufacturers' Standard Gauge
How each weight is worked
- Steel: Defined by weight: the U.S. Standard Gauge weight per square foot.
- Aluminum: For 6061 at 0.0975 lb/in³ (datasheets span 0.0975–0.0980).
Sources
Sources6
- 15 U.S.C. § 206, Standard gauge for sheet and plate iron and steel (the weights) (archived Oct 13, 2026)
- Math: American Wire Gauge (ASTM B258) is defined by 0.005" × 92^((36 − n) / 39), exact by definition (cited, not counted)
- Wikipedia, Sheet metal: gauge table (steel column from Machinery's Handbook, 27th ed.) (archived Oct 21, 2026)
- Protolabs, Aluminum 6061-T651/T6 material data sheet
- Smiths Advanced Metals, 6061 aluminium sheet (archived Nov 16, 2026)
- Alabama Specialty Products, alloy density table (A96061 Al 6061) (archived Oct 14, 2026)