Sheet metal gauge
7 gauge sheet metal thickness
7 gauge sheet metal is 0.1793" (4.56 mm) in steel, 0.1875" (4.76 mm) stainless and 0.1443" (3.66 mm) aluminum. Each metal has its own gauge system, and gauge is nominal: measure the stock when the thickness matters.
Steel
0.1793"
4.56 mm
Manufacturers' Standard Gauge
Stainless steel
0.1875"
4.76 mm
U.S. Standard Gauge
Aluminum
0.1443"
3.66 mm
Brown & Sharpe (AWG)
Checked against 3 published copies
Weight
| Material | lb/ft² | kg/m² |
|---|---|---|
| Steel | 7.500 | 36.62 |
| Stainless steel | 7.695 | 37.57 |
| Aluminum | 2.027 | 9.90 |
From the standard, Manufacturers' Standard Gauge
How each weight is worked
- Steel: Defined by weight: the U.S. Standard Gauge weight per square foot.
- Stainless steel: For 304 at 0.285 lb/in³ (datasheets span 0.285–0.290).
- Aluminum: For 6061 at 0.0975 lb/in³ (datasheets span 0.0975–0.0980).
Sources
Sources13
- 15 U.S.C. § 206, Standard gauge for sheet and plate iron and steel (the weights) (archived Oct 13, 2026)
- 15 U.S.C. § 206, Standard gauge for sheet and plate iron and steel (archived Oct 13, 2026)
- Math: American Wire Gauge (ASTM B258) is defined by 0.005" × 92^((36 − n) / 39), exact by definition (cited, not counted)
- Wikipedia, Sheet metal: gauge table (steel column from Machinery's Handbook, 27th ed.) (archived Oct 21, 2026)
- Metal Supermarkets, Sheet metal gauge chart (archived Sep 30, 2026)
- American Steel & Aluminum, Sheet metal gauge chart (archived Nov 13, 2026)
- Welders Supply, Metal gauge to thickness chart (archived Sep 8, 2026)
- Cleveland-Cliffs, 304/304L stainless product data bulletin (archived Nov 15, 2026)
- Rolled Alloys, 304/304L stainless steel data sheet (archived May 13, 2025)
- Outokumpu, 304/304L data sheet (Imperial, Americas) (archived Nov 2, 2026)
- Protolabs, Aluminum 6061-T651/T6 material data sheet
- Smiths Advanced Metals, 6061 aluminium sheet (archived Nov 16, 2026)
- Alabama Specialty Products, alloy density table (A96061 Al 6061) (archived Oct 14, 2026)