Lathe threading · 60° thread
3.5 mm pitch threading: depth and passes
Single-point a 3.5 mm pitch thread in 14 passes: 2.147 mm deep outside (2.467 mm on a compound at 29.5°), 1.894 mm inside. First pass 0.326 mm, last 0.084 mm. Fanuc G76, external: P2147 Q326.
Outside (shaft)
2.147 mm
14 passes
Inside (bore)
1.894 mm
14 passes
Only two makers publish this: Kennametal and Carmex
External thread (on a shaft): each of the 14 passes
| Pass | Cut (radial) | Total depth | Compound at 29.5° |
|---|---|---|---|
| 1 | 0.326 mm | 0.326 mm | 0.375 mm |
| 2 | 0.269 mm | 0.595 mm | 0.684 mm |
| 3 | 0.247 mm | 0.842 mm | 0.968 mm |
| 4 | 0.189 mm | 1.031 mm | 1.185 mm |
| 5 | 0.160 mm | 1.191 mm | 1.368 mm |
| 6 | 0.141 mm | 1.332 mm | 1.530 mm |
| 7 | 0.127 mm | 1.459 mm | 1.676 mm |
| 8 | 0.117 mm | 1.575 mm | 1.810 mm |
| 9 | 0.109 mm | 1.684 mm | 1.935 mm |
| 10 | 0.102 mm | 1.786 mm | 2.053 mm |
| 11 | 0.097 mm | 1.883 mm | 2.164 mm |
| 12 | 0.092 mm | 1.975 mm | 2.269 mm |
| 13 | 0.088 mm | 2.063 mm | 2.370 mm |
| 14 | 0.084 mm | 2.147 mm | 2.467 mm |
Internal thread (in a bore): each of the 14 passes
| Pass | Cut (radial) | Total depth | Compound at 29.5° |
|---|---|---|---|
| 1 | 0.288 mm | 0.288 mm | 0.331 mm |
| 2 | 0.238 mm | 0.525 mm | 0.604 mm |
| 3 | 0.218 mm | 0.743 mm | 0.854 mm |
| 4 | 0.167 mm | 0.910 mm | 1.046 mm |
| 5 | 0.141 mm | 1.051 mm | 1.207 mm |
| 6 | 0.124 mm | 1.175 mm | 1.350 mm |
| 7 | 0.112 mm | 1.287 mm | 1.479 mm |
| 8 | 0.103 mm | 1.390 mm | 1.597 mm |
| 9 | 0.096 mm | 1.486 mm | 1.707 mm |
| 10 | 0.090 mm | 1.576 mm | 1.811 mm |
| 11 | 0.085 mm | 1.662 mm | 1.909 mm |
| 12 | 0.081 mm | 1.743 mm | 2.002 mm |
| 13 | 0.077 mm | 1.820 mm | 2.091 mm |
| 14 | 0.074 mm | 1.894 mm | 2.177 mm |
G76 numbers (Fanuc two-line)
External: thread height P2147, first cut Q326. Internal: P1894,Q288. In µm, written with no decimal point. The control shrinks each pass after the first the same way as the table.
Why each pass cuts less
The √x rule, and the smallest pass
A threading tool cuts on a V, so as it goes deeper more of its edge is in the cut. Taking the same depth every pass would load the last passes far harder than the first. Sandvik’s rule, used here, makes the total depth after pass x grow with √x, so every pass removes about the same area of chip. Passes are the makers’ counts for this pitch, and none is under 0.05 mm (Kennametal), or the tool rubs instead of cutting.
Sources
Sources5
- Kennametal — Threading technical data: infeed passes, minimum infeed, infeed angle (archived Jul 28, 2026)
- Carmex — Thread turning inserts technical section: recommended cutting speed (p. 56) and number of passes (p. 58) (archived Nov 13, 2026)
- Sandvik Coromant — Turning Tools 2020 catalogue, CoroCut XS cutting data: threading infeed recommendations (p. B136) (archived Nov 15, 2026)
- Sandvik Coromant — Threading formulas and definitions (infeed per pass) (archived Oct 6, 2026)
- Peter Smid — CNC Programming Handbook, threading on CNC lathes (thread depth constants) (archived Dec 21, 2017)