Lathe threading · 60° thread
3 mm pitch threading: depth and passes
Single-point a 3 mm pitch thread in 12 passes: 1.840 mm deep outside (2.114 mm on a compound at 29.5°), 1.624 mm inside. First pass 0.304 mm, last 0.086 mm. Fanuc G76, external: P1840 Q304.
Outside (shaft)
1.840 mm
12 passes
Inside (bore)
1.624 mm
12 passes
Only two makers publish this: Kennametal and Carmex
External thread (on a shaft): each of the 12 passes
| Pass | Cut (radial) | Total depth | Compound at 29.5° |
|---|---|---|---|
| 1 | 0.304 mm | 0.304 mm | 0.349 mm |
| 2 | 0.251 mm | 0.555 mm | 0.638 mm |
| 3 | 0.230 mm | 0.785 mm | 0.902 mm |
| 4 | 0.176 mm | 0.961 mm | 1.104 mm |
| 5 | 0.149 mm | 1.110 mm | 1.275 mm |
| 6 | 0.131 mm | 1.241 mm | 1.426 mm |
| 7 | 0.118 mm | 1.359 mm | 1.562 mm |
| 8 | 0.109 mm | 1.468 mm | 1.687 mm |
| 9 | 0.101 mm | 1.569 mm | 1.803 mm |
| 10 | 0.095 mm | 1.665 mm | 1.913 mm |
| 11 | 0.090 mm | 1.755 mm | 2.016 mm |
| 12 | 0.086 mm | 1.840 mm | 2.114 mm |
Internal thread (in a bore): each of the 12 passes
| Pass | Cut (radial) | Total depth | Compound at 29.5° |
|---|---|---|---|
| 1 | 0.268 mm | 0.268 mm | 0.308 mm |
| 2 | 0.221 mm | 0.490 mm | 0.563 mm |
| 3 | 0.203 mm | 0.692 mm | 0.796 mm |
| 4 | 0.156 mm | 0.848 mm | 0.974 mm |
| 5 | 0.131 mm | 0.979 mm | 1.125 mm |
| 6 | 0.116 mm | 1.095 mm | 1.258 mm |
| 7 | 0.104 mm | 1.199 mm | 1.378 mm |
| 8 | 0.096 mm | 1.295 mm | 1.488 mm |
| 9 | 0.089 mm | 1.385 mm | 1.591 mm |
| 10 | 0.084 mm | 1.469 mm | 1.688 mm |
| 11 | 0.079 mm | 1.548 mm | 1.779 mm |
| 12 | 0.076 mm | 1.624 mm | 1.866 mm |
G76 numbers (Fanuc two-line)
External: thread height P1840, first cut Q304. Internal: P1624,Q268. In µm, written with no decimal point. The control shrinks each pass after the first the same way as the table.
Why each pass cuts less
The √x rule, and the smallest pass
A threading tool cuts on a V, so as it goes deeper more of its edge is in the cut. Taking the same depth every pass would load the last passes far harder than the first. Sandvik’s rule, used here, makes the total depth after pass x grow with √x, so every pass removes about the same area of chip. Passes are the makers’ counts for this pitch, and none is under 0.05 mm (Kennametal), or the tool rubs instead of cutting.
Sources
Sources5
- Kennametal — Threading technical data: infeed passes, minimum infeed, infeed angle (archived Jul 28, 2026)
- Carmex — Thread turning inserts technical section: recommended cutting speed (p. 56) and number of passes (p. 58) (archived Nov 13, 2026)
- Sandvik Coromant — Turning Tools 2020 catalogue, CoroCut XS cutting data: threading infeed recommendations (p. B136) (archived Nov 15, 2026)
- Sandvik Coromant — Threading formulas and definitions (infeed per pass) (archived Oct 6, 2026)
- Peter Smid — CNC Programming Handbook, threading on CNC lathes (thread depth constants) (archived Dec 21, 2017)