ISO 286 · Hole
G10 hole tolerance
G10 tolerance on a 25 mm hole is +0.091 / +0.007 mm, so the hole measures 25.007–25.091 mm. A G hole sits wholly above the nominal size, so it clears an h shaft. Grade 10 (IT10) sets the band’s width; the chart below gives it for every size to 500 mm.
g10 shaft on 25 mm: −0.007 / −0.091 mm. g10 shaft tolerance
Limits by size
Deviations from the nominal size, over the first size up to and including the second. Inches are µm ÷ 25,400; ANSI B4.2 inch tables round differently, by a tenth or so.
| Size, mm | Upper µm | Lower µm | Upper in | Lower in |
|---|---|---|---|---|
| 0–3 | +42 | +2 | +0.00165 | +0.00008 |
| 3–6 | +52 | +4 | +0.00205 | +0.00016 |
| 6–10 | +63 | +5 | +0.00248 | +0.00020 |
| 10–18 | +76 | +6 | +0.00299 | +0.00024 |
| 18–30 | +91 | +7 | +0.00358 | +0.00028 |
| 30–50 | +109 | +9 | +0.00429 | +0.00035 |
| 50–80 | +130 | +10 | +0.00512 | +0.00039 |
| 80–120 | +152 | +12 | +0.00598 | +0.00047 |
| 120–180 | +174 | +14 | +0.00685 | +0.00055 |
| 180–250 | +200 | +15 | +0.00787 | +0.00059 |
| 250–315 | +227 | +17 | +0.00894 | +0.00067 |
| 315–400 | +248 | +18 | +0.00976 | +0.00071 |
| 400–500 | +270 | +20 | +0.01063 | +0.00079 |
Checked against 3 published copies
Sources
Sources3
ISO 286-1 and 286-2. Every limit on this page was checked against these published copies of the tables: