ISO 286 · Hole
G9 hole tolerance
G9 tolerance on a 25 mm hole is +0.059 / +0.007 mm, so the hole measures 25.007–25.059 mm. A G hole sits wholly above the nominal size, so it clears an h shaft. Grade 9 (IT9) sets the band’s width; the chart below gives it for every size to 500 mm.
g9 shaft on 25 mm: −0.007 / −0.059 mm. g9 shaft tolerance
Limits by size
Deviations from the nominal size, over the first size up to and including the second. Inches are µm ÷ 25,400; ANSI B4.2 inch tables round differently, by a tenth or so.
| Size, mm | Upper µm | Lower µm | Upper in | Lower in |
|---|---|---|---|---|
| 0–3 | +27 | +2 | +0.00106 | +0.00008 |
| 3–6 | +34 | +4 | +0.00134 | +0.00016 |
| 6–10 | +41 | +5 | +0.00161 | +0.00020 |
| 10–18 | +49 | +6 | +0.00193 | +0.00024 |
| 18–30 | +59 | +7 | +0.00232 | +0.00028 |
| 30–50 | +71 | +9 | +0.00280 | +0.00035 |
| 50–80 | +84 | +10 | +0.00331 | +0.00039 |
| 80–120 | +99 | +12 | +0.00390 | +0.00047 |
| 120–180 | +114 | +14 | +0.00449 | +0.00055 |
| 180–250 | +130 | +15 | +0.00512 | +0.00059 |
| 250–315 | +147 | +17 | +0.00579 | +0.00067 |
| 315–400 | +158 | +18 | +0.00622 | +0.00071 |
| 400–500 | +175 | +20 | +0.00689 | +0.00079 |
Checked against 3 published copies
Sources
Sources3
ISO 286-1 and 286-2. Every limit on this page was checked against these published copies of the tables: