ISO 286 · Hole

G8 hole tolerance

G8 tolerance on a 25 mm hole is +0.040 / +0.007 mm, so the hole measures 25.007–25.040 mm. A G hole sits wholly above the nominal size, so it clears an h shaft. Grade 8 (IT8) sets the band’s width; the chart below gives it for every size to 500 mm.

g8 shaft on 25 mm: −0.007 / −0.040 mm. g8 shaft tolerance

G8 hole tolerance zone for every size range from 0–3 mm to 400–500 mm, against the zero line; 18–30 mm is +40 / +7 µm.tolerance zone G8, 18–30 mm: +40 / +7 µmsize range 0–3 to 400–500 mm
One band per size range against the zero line. The marked band holds 25 mm. Deviations to scale; the size ranges are evenly spaced, not to scale.

Limits by size

Deviations from the nominal size, over the first size up to and including the second. Inches are µm ÷ 25,400; ANSI B4.2 inch tables round differently, by a tenth or so.

G8 limits by nominal size
Size, mmUpper µmLower µmUpper inLower in
0–3+16+2+0.00063+0.00008
3–6+22+4+0.00087+0.00016
6–10+27+5+0.00106+0.00020
10–18+33+6+0.00130+0.00024
18–30+40+7+0.00157+0.00028
30–50+48+9+0.00189+0.00035
50–80+56+10+0.00220+0.00039
80–120+66+12+0.00260+0.00047
120–180+77+14+0.00303+0.00055
180–250+87+15+0.00343+0.00059
250–315+98+17+0.00386+0.00067
315–400+107+18+0.00421+0.00071
400–500+117+20+0.00461+0.00079

Checked against 3 published copies

Any size and fit in the calculator

Sources

Sources3