Holes wander off position or run crooked
Mitsubishi and OSG both say: regrind the point so both lips match, and check it after grinding; check runout at the holder, or use another holder, and check again once the drill is clamped; use a point thinning that cuts with less force, or spot the hole first.
What you see
Holes land off position, lean out of square, or run off line in a deep hole.
Causes and what to change
Every fix here is from Mitsubishi and OSG's troubleshooting guides, unless marked. Change one thing at a time.
A point ground unevenly: lip heights that differ, or a chisel edge off center
Regrind the point so both lips match, and check it after grinding
Runout at the holder or the spindle
Check runout at the holder, or use another holder, and check again once the drill is clamped
The drill walking as it enters the work
Use a point thinning that cuts with less force, or spot the hole first
Use a stiffer drill and machine, clamp the work stiffer, and guide the drill with a bushing
Only OSG
Feed too high on entry
Lower the feed as the drill enters
Only Mitsubishi
Work it out: Drilling speeds and feeds calculator
Flutes longer than the hole needs
Use a drill with shorter flutes
Only Mitsubishi
A pilot hole that is off, or too shallow
Drill the pilot hole true, and deeper
Only Mitsubishi
A surface that isn’t square to the drill
Make a center hole, with the work square to the drill
Only OSG
Poor alignment on a lathe
Check the alignment
Only OSG
A drill that isn’t stiff enough
Use a stiffer drill
Only OSG
A worn drill
Regrind the worn drill
Only OSG
Work it out
Often comes with
Sources
Sources2
- Mitsubishi Materials — Drilling course: Trouble shooting
- OSG — Drilling Technical Guide, Part 8: Troubleshooting (pp. 34–35)
Written in our own words from each maker's troubleshooting guide.