Kennametal · chipbreaker for negative inserts
FP chipbreaker
Finishing stainless.
One source: Kennametal, its own catalog
What Kennametal prints
- Insert
- Negative
- Made for
- ISO M (stainless steel)
- Cutting area
- finishing
- Feed
- 0.1–0.3 mm/rev (.0039–.0118 in/rev)
- Depth of cut
- 0.25–2.54 mm (.01–.10 in)
Kennametal prints its windows in inches; the millimetres are converted (×25.4, two places).
Source: Kennametal — Master Catalog 2018, Vol. 1 Turning Tools (inch), chip control geometries (pp. B30–B35) (archived Jun 4, 2023)
FP equivalents
Other makers’ chipbreakers for negative inserts that their own catalogs make for at least one of the same main ISO groups and cutting areas. Equivalent means the same job, not the same shape: check the feed window for your cut.
| Maker | Chipbreaker | In common | Feed | What its maker says | Source |
|---|---|---|---|---|---|
| Sandvik | MF | ISO M; finishing | not printed | First choice for finishing stainless (T-Max P). | One source: Sandvik Coromant, its own catalog |
| Seco | MF1 | ISO M; finishing | 0.08–0.3 mm/rev | Semi-finishing and finishing of stainless, superalloys and titanium. | One source: Seco Tools, its own catalog |
| Seco | MF4 | ISO M; finishing | 0.15–0.5 mm/rev | Medium and finishing cuts in stainless. | One source: Seco Tools, its own catalog |
| Seco | MF5 | ISO M; finishing | 0.2–0.8 mm/rev | Medium finishing of steel and stainless at high feeds. | One source: Seco Tools, its own catalog |
Why FP for austenitic stainless (304, 316)
FP for austenitic stainless (304, 316): Kennametal’s finishing geometry for ISO M.
The reasoning, step by step
The situation
Austenitic stainless work-hardens as it is cut, conducts heat poorly and sticks to the edge. The hardened skin and chips wear a notch in the edge at the depth-of-cut line.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
What that means
A work-hardening alloy needs a sharp, positive edge, and a feed and depth that cut under the layer the last pass hardened. An edge that rubs hardens the next layer.
Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]
So
Kennametal makes FP (negative) for M in finishing at 0.1–0.3 mm/rev (.0039–.0118 in/rev). Finishing stainless.
One source: Kennametal, the maker of the chipbreaker , sources [4]
- Sandvik Coromant — Workpiece materials: ISO M stainless
- Mitsubishi Materials — Machining course: ISO group M, stainless steel
- NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
- Kennametal — Master Catalog 2018, Vol. 1 Turning Tools (inch), chip control geometries (pp. B30–B35) (archived Jun 4, 2023)
What the cross-reference says
Mitsubishi’s chipbreaker comparison table, a compilation, lists FP for ISO M, finishing. Kennametal’s own catalog is the authority for its geometry.
It agrees with Kennametal’s catalog.
Source: Mitsubishi Materials USA — Insert Chip Breaker Comparison Table (archived Jul 14, 2024)