Lathe

Insert grade picker

The grade and chipbreaker makers recommend for your material and cut, with each maker's equivalent.

Steel, gray iron, austenitic stainless, superalloys and titanium are covered so far.
Operation
Cut
Setup
Units

Grade

MC7025

CVD TiCN-Al2O3-TiN, thin · M30

One source: Mitsubishi Materials, its own catalog

Chipbreaker

MM

Negative insert

One source: Mitsubishi Materials, its own catalog

Mitsubishi MM and its equivalents

Nose radius

1/32″

0.8 mm · sized to the starting feed

Why: 304 work-hardens and holds heat: Mitsubishi MC7025 with the MM breaker, a 0.8 mm nose radius, starting at 551 SFM.

Surface speed

551SFM

Window 295 – 787

Median of 6 makers

Feed

.0120in/rev

Window .0036 – .0178

Median of 5 makers

Each maker’s equivalent

Grades whose maker rates them for M30 in its own catalog, the same coating family first.

Equivalent grades by maker
MakerGradeCoatingMaker’s rangeSource
MitsubishiMC7025CVD TiCN-Al2O3-TiN, thinM20–M40

One source: Mitsubishi Materials, its own catalog

ISCARIC635CVD TiN + TiC + TiNM20–M40

One source: ISCAR, its own catalog

KennametalKCM25CVD Multilayer MTCVD TiCN-Al2O3M20–M30

One source: Kennametal, its own catalog

SandvikGC2025CVDM15–M35

One source: Sandvik Coromant, its own catalog

SecoTM3501CVD Ti(C,N) + Al2O3, chrome used-edge detection layerabout M25–M35

One source: Seco Tools, its own catalog

Chipbreakers for the same job

  • Kennametal MS: Medium machining, sharp edge, stainless and high-temperature alloys.
  • Kennametal P: Medium machining of steel, stainless and high-temperature alloys.
  • Kennametal UP: Medium machining of stainless and high-temperature alloys.
  • Sandvik MM: First choice for medium machining of stainless (T-Max P).
  • Seco M5: Roughing with double-sided inserts at high feed in steel, stainless and cast iron.
  • Seco MF4: Medium and finishing cuts in stainless.
  • Seco MF5: Medium finishing of steel and stainless at high feeds.
  • Seco MR3: Medium-rough and rough machining of superalloys, titanium, stainless and hardened steel.
Why these numbers?
  1. The situation

    Austenitic stainless work-hardens as it is cut, conducts heat poorly and sticks to the edge. The hardened skin and chips wear a notch in the edge at the depth-of-cut line.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  2. What that means

    A work-hardening alloy needs a sharp, positive edge, and a feed and depth that cut under the layer the last pass hardened. An edge that rubs hardens the next layer.

    Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]

  3. So

    Mitsubishi’s first choice for stainless steel under 200 HB (e.g. 304, 316), general conditions, a medium cut: MC7025 (CVD TiCN-Al2O3-TiN, thin; substrate: 89.4 HRA), rated M30 in Mitsubishi’s own range (M20–M40).

    One source: Mitsubishi Materials, the maker of the grade , sources [4, 5]

  4. So

    Chipbreaker MM (Mitsubishi’s first choice for this cut): First recommendation for medium cutting of stainless.

    One source: Mitsubishi Materials, the maker of the chipbreaker , sources [4, 6]

  5. So

    A larger nose radius makes a stronger edge and carries more feed, but too large a radius for the cut chatters. So the radius follows the feed: at least about twice the feed, with the feed inside that radius’s maximum. At this feed that is a 0.8 mm (1/32") nose radius.

    3 sources agree , sources [7, 8, 9]

  6. So

    A larger lead angle (a smaller entering angle, as on a round insert or a 45° holder) thins the chip and spreads the load along more edge, which reduces notch wear and lengthens tool life. The cost is more radial force, which can push a slender part or start vibration.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [7, 10]

  7. The number

    Start at 551 SFM; the makers’ window for CVD grades is 295–787 SFM.

    6 sources agree

Sources

  1. Sandvik Coromant — Workpiece materials: ISO M stainless
  2. Mitsubishi Materials — Machining course: ISO group M, stainless steel
  3. NeoNickel — Machining NeoNickel high performance alloys
  4. Mitsubishi Materials — General Catalog C010A: optimum grades and chip breakers for external turning, stainless steel (p. A016)
  5. Mitsubishi Materials — General Catalog C010A, turning inserts: grades (pp. A034–A044)
  6. Mitsubishi Materials — General Catalog C010A, turning inserts: chip breaker classification (pp. A046–A070)
  7. Sandvik Coromant — Turning Handbook C-1020-18: general turning (entering angle, nose radius)
  8. Walter — Technical Compendium, Turning 2024: feed ranges by corner radius (p. A 55)
  9. Mitsubishi Materials — Turning technical data: corner radius
  10. Mitsubishi Materials — Turning technical data: side cutting edge (lead) angle
  11. Kennametal — Turning inserts, carbide: RP, MP, FP and MS geometries, cutting speed (SFM) ranges and starting feeds
  12. Mitsubishi Materials USA — Optimum Grades and Chip Breakers for External Turning
  13. Kyocera — Recommended cutting conditions, external turning (negative inserts), catalog pp. D46–D47
  14. Tungaloy — General catalog 2023–2024, inserts: chipbreaker guide, standard cutting conditions and selection system (pp. B004–B013)
  15. Sumitomo Electric — General catalogue 2018–2019, insert selection: recommended cutting conditions (pp. A5–A12)
  16. Korloy — Turning: recommended chip breaker for workpiece, cutting speeds and feeds (pp. B4–B11)

How we source these numbers

What next

What speed and feed for this lathe cut?Lathe SFM, feed and depth of cut for your material and insert, with the RPM.
What’s wrong with this cut?Stringy chips, chatter, a torn finish, built-up edge or chipped inserts: causes and what to change.
What finish will this feed leave?The Ra a feed and nose radius leave, or the feed an Ra callout allows.
How the insert grade picker works

For a medium OD cut in 304 stainless, Mitsubishi recommends MC7025 with its MM chipbreaker, on a 0.8 mm nose radius.