Seco · chipbreaker for negative inserts
MF1 chipbreaker
Semi-finishing and finishing of stainless, superalloys and titanium.
One source: Seco Tools, its own catalog
What Seco prints
- Insert
- Negative
- Made for
- ISO M (stainless steel), S (superalloys and titanium)
- Cutting area
- finishing, light cuts
- Feed
- 0.08–0.3 mm/rev (.0031–.0118 in/rev)
- Depth of cut
- 0.2–3.5 mm (.008–.138 in)
- Edge
- Sharp ground (.GG) or lightly honed (.MG)
Source: Seco Tools — Turning catalogue 2026.2: carbide chipbreakers (pp. 111–114) (archived Nov 16, 2026)
MF1 equivalents
Other makers’ chipbreakers for negative inserts that their own catalogs make for at least one of the same main ISO groups and cutting areas. Equivalent means the same job, not the same shape: check the feed window for your cut.
| Maker | Chipbreaker | In common | Feed | What its maker says | Source |
|---|---|---|---|---|---|
| Kennametal | FP | ISO M; finishing | 0.1–0.3 mm/rev | Finishing stainless. | One source: Kennametal, its own catalog |
| Kennametal | FS | ISO S; finishing | 0.08–0.25 mm/rev | Sharp finishing of high-temperature alloys. | One source: Kennametal, its own catalog |
| Kennametal | LF | ISO M, S; finishing | 0.13–0.51 mm/rev | Finishing stainless and high-temperature alloys. | One source: Kennametal, its own catalog |
| Mitsubishi | FJ | ISO S; finishing | not printed | Alternative for finishing heat resistant and titanium alloys. | One source: Mitsubishi Materials, its own catalog |
| Mitsubishi | FS | ISO S; finishing | not printed | Finishing difficult-to-cut materials (G class); the M-class FS is an alternative for finishing mild steel. | One source: Mitsubishi Materials, its own catalog |
| Mitsubishi | GM | ISO M; light cuts | not printed | Alternative to LM and MM for stainless; notch-wear resistant for light to medium cuts. | One source: Mitsubishi Materials, its own catalog |
| Mitsubishi | LM | ISO M; light cuts | not printed | First recommendation for light cutting of stainless; high rake controls burrs. | One source: Mitsubishi Materials, its own catalog |
| Mitsubishi | LS | ISO S; light cuts | not printed | First recommendation for light cutting of difficult-to-cut materials; alternative for stainless; chip control at depths under the corner radius. | One source: Mitsubishi Materials, its own catalog |
| Mitsubishi | MJ | ISO S; light cuts | not printed | Alternative for light cutting of heat resistant and titanium alloys; notch-wear resistant for light to medium cuts. | One source: Mitsubishi Materials, its own catalog |
| Sandvik | MF | ISO M; finishing | not printed | First choice for finishing stainless (T-Max P). | One source: Sandvik Coromant, its own catalog |
Why MF1 for austenitic stainless (304, 316)
MF1 for austenitic stainless (304, 316): Seco’s finishing and light cuts geometry for ISO M.
The reasoning, step by step
The situation
Austenitic stainless work-hardens as it is cut, conducts heat poorly and sticks to the edge. The hardened skin and chips wear a notch in the edge at the depth-of-cut line.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
What that means
A work-hardening alloy needs a sharp, positive edge, and a feed and depth that cut under the layer the last pass hardened. An edge that rubs hardens the next layer.
Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]
So
Seco makes MF1 (negative) for M, S in finishing, light cuts at 0.08–0.3 mm/rev (.0031–.0118 in/rev); edge: Sharp ground (.GG) or lightly honed (.MG). Semi-finishing and finishing of stainless, superalloys and titanium.
One source: Seco Tools, the maker of the chipbreaker , sources [4]
- Sandvik Coromant — Workpiece materials: ISO M stainless
- Mitsubishi Materials — Machining course: ISO group M, stainless steel
- NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
- Seco Tools — Turning catalogue 2026.2: carbide chipbreakers (pp. 111–114) (archived Nov 16, 2026)
What the cross-reference says
Mitsubishi’s chipbreaker comparison table, a compilation, lists MF1 for ISO M, S, finishing. Seco Tools’ own catalog is the authority for its geometry.
It agrees with Seco Tools’ catalog.
Source: Mitsubishi Materials USA — Insert Chip Breaker Comparison Table (archived Jul 14, 2024)