Kennametal · chipbreaker for positive inserts

HP chipbreaker

Finishing cast iron, non-ferrous and high-temperature alloys.

One source: Kennametal, its own catalog

The cutting edge of a positive insert in section: the breaker groove behind the edge with a chip curling out of it, and the flank at 7° clearance; made for ISO K, N and S.chipcutting edgebreaker grooveclearance 7°ISO groupKNS
The edge in section; its ISO groups. Not to scale.

What Kennametal prints

Insert
Positive
Made for
ISO K (cast iron), N (non-ferrous), S (superalloys and titanium)
Cutting area
finishing
Feed
0.18–0.38 mm/rev (.0071–.015 in/rev)
Depth of cut
0.64–2.29 mm (.025–.09 in)
Edge
Precision ground

Kennametal prints its windows in inches; the millimetres are converted (×25.4, two places).

Source: Kennametal — Master Catalog 2018, Vol. 1 Turning Tools (inch), chip control geometries (pp. B30–B35) (archived Jun 4, 2023)

HP equivalents

Other makers’ chipbreakers for positive inserts that their own catalogs make for at least one of the same main ISO groups and cutting areas. Equivalent means the same job, not the same shape: check the feed window for your cut.

Other makers’ chipbreakers for the same job
MakerChipbreakerIn commonFeedWhat its maker saysSource
MitsubishiAZISO N; finishingnot printedAluminum alloys: a sharp point and chip control from the 3D rake face; the lapped top face resists welding.

One source: Mitsubishi Materials, its own catalog

MitsubishiFJISO S; finishingnot printedFinishing difficult-to-cut materials.

One source: Mitsubishi Materials, its own catalog

MitsubishiFSISO S; finishingnot printedFirst recommendation for finishing heat resistant, titanium and cobalt-chrome alloys.

One source: Mitsubishi Materials, its own catalog

MitsubishiFS-PISO S; finishingnot printedFirst recommendation for finishing titanium alloys.

One source: Mitsubishi Materials, its own catalog

MitsubishiMJISO S; finishingnot printedFinish to light cutting of heat resistant and titanium alloys.

One source: Mitsubishi Materials, its own catalog

Why HP for gray cast iron

HP for gray cast iron: Kennametal’s finishing geometry for ISO K.

The reasoning, step by step
  1. The situation

    Gray iron breaks into short chips (its graphite acts as a chipbreaker), but the hard particles in it are abrasive to the edge.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  2. So

    Kennametal makes HP (positive) for K, N, S in finishing at 0.18–0.38 mm/rev (.0071–.015 in/rev); edge: Precision ground. Finishing cast iron, non-ferrous and high-temperature alloys.

    One source: Kennametal, the maker of the chipbreaker , sources [3]

  1. Sandvik Coromant — Workpiece materials: ISO K cast iron
  2. Mitsubishi Materials — Machining course: ISO group K, cast iron
  3. Kennametal — Master Catalog 2018, Vol. 1 Turning Tools (inch), chip control geometries (pp. B30–B35) (archived Jun 4, 2023)

What the cross-reference says

Mitsubishi’s chipbreaker comparison table, a compilation, lists HP for ISO M, N, S, finishing, light cuts, medium. Kennametal’s own catalog is the authority for its geometry.

Source: Mitsubishi Materials USA — Insert Chip Breaker Comparison Table (archived Jul 14, 2024)