Mitsubishi · chipbreaker for positive inserts
FS-P chipbreaker
First recommendation for finishing titanium alloys.
One source: Mitsubishi Materials, its own catalog
What Mitsubishi prints
- Insert
- Positive
- Made for
- ISO S (superalloys and titanium)
- Cutting area
- finishing
- Edge
- Sharp, lapped top face
Source: Mitsubishi Materials — General Catalog C010A, turning inserts: chip breaker classification (pp. A046–A070) (archived Nov 15, 2026)
FS-P equivalents
Other makers’ chipbreakers for positive inserts that their own catalogs make for at least one of the same main ISO groups and cutting areas. Equivalent means the same job, not the same shape: check the feed window for your cut.
| Maker | Chipbreaker | In common | Feed | What its maker says | Source |
|---|---|---|---|---|---|
| Kennametal | FP | ISO S; finishing | 0.06–0.25 mm/rev | Finishing steel, stainless, cast iron and high-temperature alloys. | One source: Kennametal, its own catalog |
| Kennametal | HP | ISO S; finishing | 0.18–0.38 mm/rev | Finishing cast iron, non-ferrous and high-temperature alloys. | One source: Kennametal, its own catalog |
| Kennametal | LF | ISO S; finishing | not printed | Finishing: steel, stainless, cast iron (MT-LF); non-ferrous and high-temperature alloys (GT-LF, precision ground). | One source: Kennametal, its own catalog |
Why FS-P for titanium alloys
FS-P for titanium alloys: Mitsubishi’s finishing geometry for ISO S.
The reasoning, step by step
The situation
Titanium conducts heat poorly, so the heat stays in the edge instead of leaving with the chip, and its thin chips gall onto the rake face.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
So
Mitsubishi makes FS-P (positive) for S in finishing; edge: Sharp, lapped top face. First recommendation for finishing titanium alloys.
One source: Mitsubishi Materials, the maker of the chipbreaker , sources [3]
What the cross-reference says
Mitsubishi’s chipbreaker comparison table, a compilation, lists FS-P for ISO S, finishing. Mitsubishi Materials’ own catalog is the authority for its geometry.
It agrees with Mitsubishi Materials’ catalog.
Source: Mitsubishi Materials USA — Insert Chip Breaker Comparison Table (archived Jul 14, 2024)