Kennametal · chipbreaker for negative inserts

MP chipbreaker

Medium machining of steel and non-ferrous.

One source: Kennametal, its own catalog

The cutting edge of a negative insert in section: the breaker groove behind the edge with a chip curling out of it, and the flank at 0° clearance; made for ISO P and N.chipcutting edgebreaker grooveclearance 0°ISO groupPN
The edge in section; its ISO groups. Not to scale.

What Kennametal prints

Insert
Negative
Made for
ISO P (steel), N (non-ferrous)
Cutting area
medium
Feed
0.15–0.51 mm/rev (.0059–.0201 in/rev)
Depth of cut
0.76–5.08 mm (.03–.20 in)

Kennametal prints its windows in inches; the millimetres are converted (×25.4, two places).

Source: Kennametal — Master Catalog 2018, Vol. 1 Turning Tools (inch), chip control geometries (pp. B30–B35) (archived Jun 4, 2023)

MP equivalents

Other makers’ chipbreakers for negative inserts that their own catalogs make for at least one of the same main ISO groups and cutting areas. Equivalent means the same job, not the same shape: check the feed window for your cut.

Other makers’ chipbreakers for the same job
MakerChipbreakerIn commonFeedWhat its maker saysSource
MitsubishiMPISO P; medium0.15–0.51 mm/revFirst recommendation for medium cutting of carbon and alloy steel; also light cutting, copying and back turning.

One source: Mitsubishi Materials, its own catalog

SecoM5ISO P; medium0.3–0.7 mm/revRoughing with double-sided inserts at high feed in steel, stainless and cast iron.

One source: Seco Tools, its own catalog

SecoMF5ISO P; medium0.2–0.8 mm/revMedium finishing of steel and stainless at high feeds.

One source: Seco Tools, its own catalog

Why MP for steel

MP for steel: Kennametal’s medium geometry for ISO P.

The reasoning, step by step
  1. The situation

    Steel makes chips that are fairly easy to control. The edge’s main enemy is heat, and the harder or higher in carbon the steel, the hotter the edge runs.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  2. So

    Kennametal makes MP (negative) for P, N in medium at 0.15–0.51 mm/rev (.0059–.0201 in/rev). Medium machining of steel and non-ferrous.

    One source: Kennametal, the maker of the chipbreaker , sources [3]

  1. Sandvik Coromant — Workpiece materials: ISO P steel
  2. Mitsubishi Materials — Machining course: ISO group P, steel
  3. Kennametal — Master Catalog 2018, Vol. 1 Turning Tools (inch), chip control geometries (pp. B30–B35) (archived Jun 4, 2023)

What the cross-reference says

Mitsubishi’s chipbreaker comparison table, a compilation, lists MP for ISO M, medium. Kennametal’s own catalog is the authority for its geometry.

Source: Mitsubishi Materials USA — Insert Chip Breaker Comparison Table (archived Jul 14, 2024)