Seco · chipbreaker for negative inserts

M5 chipbreaker

Roughing with double-sided inserts at high feed in steel, stainless and cast iron.

One source: Seco Tools, its own catalog

The cutting edge of a negative insert in section: the breaker groove behind the edge with a chip curling out of it, and the flank at 0° clearance; made for ISO P, M and K.chipcutting edgebreaker grooveclearance 0°ISO groupPMK
The edge in section; its ISO groups. Not to scale.

What Seco prints

Insert
Negative
Made for
ISO P (steel), M (stainless steel), K (cast iron)
Cutting area
medium, roughing, heavy roughing
Feed
0.3–0.7 mm/rev (.0118–.0276 in/rev)
Depth of cut
1.5–7 mm (.059–.276 in)

Source: Seco Tools — Turning catalogue 2026.2: carbide chipbreakers (pp. 111–114) (archived Nov 16, 2026)

M5 equivalents

Other makers’ chipbreakers for negative inserts that their own catalogs make for at least one of the same main ISO groups and cutting areas. Equivalent means the same job, not the same shape: check the feed window for your cut.

Other makers’ chipbreakers for the same job
MakerChipbreakerIn commonFeedWhat its maker saysSource
KennametalMPISO P; medium0.15–0.51 mm/revMedium machining of steel and non-ferrous.

One source: Kennametal, its own catalog

KennametalMSISO M; medium0.13–0.36 mm/revMedium machining, sharp edge, stainless and high-temperature alloys.

One source: Kennametal, its own catalog

KennametalPISO P, M; medium0.15–0.51 mm/revMedium machining of steel, stainless and high-temperature alloys.

One source: Kennametal, its own catalog

KennametalRPISO P, M, K; roughing, heavy roughingnot printedRoughing stainless (MG-RP, double-sided); heavy roughing of steel, stainless and cast iron (MM-RP, single-sided).

One source: Kennametal, its own catalog

KennametalUPISO M; medium0.2–0.64 mm/revMedium machining of stainless and high-temperature alloys.

One source: Kennametal, its own catalog

MitsubishiESISO M; mediumnot printedRight- or left-hand alternative for medium cutting of stainless.

One source: Mitsubishi Materials, its own catalog

MitsubishiGHISO P, K; roughingnot printedAlternative for rough cutting of steel and cast iron; interrupted cuts and scale.

One source: Mitsubishi Materials, its own catalog

MitsubishiGMISO M; mediumnot printedAlternative to LM and MM for stainless; notch-wear resistant for light to medium cuts.

One source: Mitsubishi Materials, its own catalog

MitsubishiHLISO M; heavy roughingnot printedFirst recommendation for heavy cutting of stainless; alternative for steel.

One source: Mitsubishi Materials, its own catalog

MitsubishiHZISO P; heavy roughingnot printedAlternative for heavy cutting of carbon and alloy steel.

One source: Mitsubishi Materials, its own catalog

Show 8 more equivalents
More of other makers’ chipbreakers for the same job
MakerChipbreakerIn commonFeedWhat its maker saysSource
MitsubishiMKISO K; medium0.2–0.56 mm/revFirst recommendation for medium cutting of cast iron; balances sharpness and edge strength.

One source: Mitsubishi Materials, its own catalog

MitsubishiMMISO M; medium0.15–0.46 mm/revFirst recommendation for medium cutting of stainless.

One source: Mitsubishi Materials, its own catalog

MitsubishiMPISO P; medium0.15–0.51 mm/revFirst recommendation for medium cutting of carbon and alloy steel; also light cutting, copying and back turning.

One source: Mitsubishi Materials, its own catalog

MitsubishiRKISO K; roughingnot printedFirst recommendation for rough cutting of cast iron; stable in interrupted cuts and scale removal.

One source: Mitsubishi Materials, its own catalog

MitsubishiRMISO M; roughingnot printedFirst recommendation for rough cutting of stainless; resists fracture in interrupted cuts.

One source: Mitsubishi Materials, its own catalog

MitsubishiRPISO P; roughingnot printedFirst recommendation for rough cutting of carbon and alloy steel; interrupted cuts and removing scale.

One source: Mitsubishi Materials, its own catalog

SandvikMMISO M; mediumnot printedFirst choice for medium machining of stainless (T-Max P).

One source: Sandvik Coromant, its own catalog

SandvikMRISO M; roughingnot printedFirst choice for roughing stainless (T-Max P).

One source: Sandvik Coromant, its own catalog

Why M5 for steel

M5 for steel: Seco’s medium and roughing and heavy roughing geometry for ISO P.

The reasoning, step by step
  1. The situation

    Steel makes chips that are fairly easy to control. The edge’s main enemy is heat, and the harder or higher in carbon the steel, the hotter the edge runs.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  2. So

    Seco makes M5 (negative) for P, M, K in medium, roughing, heavy roughing at 0.3–0.7 mm/rev (.0118–.0276 in/rev). Roughing with double-sided inserts at high feed in steel, stainless and cast iron.

    One source: Seco Tools, the maker of the chipbreaker , sources [3]

  1. Sandvik Coromant — Workpiece materials: ISO P steel
  2. Mitsubishi Materials — Machining course: ISO group P, steel
  3. Seco Tools — Turning catalogue 2026.2: carbide chipbreakers (pp. 111–114) (archived Nov 16, 2026)

What the cross-reference says

Mitsubishi’s chipbreaker comparison table, a compilation, lists M5 for ISO P, M, K, medium, roughing, heavy roughing. Seco Tools’ own catalog is the authority for its geometry.

It agrees with Seco Tools’ catalog.

Source: Mitsubishi Materials USA — Insert Chip Breaker Comparison Table (archived Jul 14, 2024)