Kennametal · chipbreaker for positive inserts

UF chipbreaker

Fine finishing of steel, stainless and cast iron.

One source: Kennametal, its own catalog

The cutting edge of a positive insert in section: the breaker groove behind the edge with a chip curling out of it, and the flank at 7° clearance; made for ISO P, M and K.chipcutting edgebreaker grooveclearance 7°ISO groupPMK
The edge in section; its ISO groups. Not to scale.

What Kennametal prints

Insert
Positive
Made for
ISO P (steel), M (stainless steel), K (cast iron)
Cutting area
finishing
Feed
0.05–0.25 mm/rev (.002–.0098 in/rev)
Depth of cut
0.13–1.27 mm (.005–.05 in)

Kennametal prints its windows in inches; the millimetres are converted (×25.4, two places).

Source: Kennametal — Master Catalog 2018, Vol. 1 Turning Tools (inch), chip control geometries (pp. B30–B35) (archived Jun 4, 2023)

UF equivalents

Other makers’ chipbreakers for positive inserts that their own catalogs make for at least one of the same main ISO groups and cutting areas. Equivalent means the same job, not the same shape: check the feed window for your cut.

Other makers’ chipbreakers for the same job
MakerChipbreakerIn commonFeedWhat its maker saysSource
MitsubishiFMISO M; finishingnot printedFirst recommendation for finishing stainless.

One source: Mitsubishi Materials, its own catalog

SandvikMFISO M; finishingnot printedFirst choice for finishing stainless (CoroTurn 107).

One source: Sandvik Coromant, its own catalog

Why UF for steel

UF for steel: Kennametal’s finishing geometry for ISO P.

The reasoning, step by step
  1. The situation

    Steel makes chips that are fairly easy to control. The edge’s main enemy is heat, and the harder or higher in carbon the steel, the hotter the edge runs.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  2. So

    Kennametal makes UF (positive) for P, M, K in finishing at 0.05–0.25 mm/rev (.002–.0098 in/rev). Fine finishing of steel, stainless and cast iron.

    One source: Kennametal, the maker of the chipbreaker , sources [3]

  1. Sandvik Coromant — Workpiece materials: ISO P steel
  2. Mitsubishi Materials — Machining course: ISO group P, steel
  3. Kennametal — Master Catalog 2018, Vol. 1 Turning Tools (inch), chip control geometries (pp. B30–B35) (archived Jun 4, 2023)

What the cross-reference says

Mitsubishi’s chipbreaker comparison table, a compilation, lists UF for ISO P, M, finishing. Kennametal’s own catalog is the authority for its geometry.

It agrees with Kennametal’s catalog.

Source: Mitsubishi Materials USA — Insert Chip Breaker Comparison Table (archived Jul 14, 2024)