Mitsubishi · chipbreaker for positive inserts

FM chipbreaker

First recommendation for finishing stainless.

One source: Mitsubishi Materials, its own catalog

The cutting edge of a positive insert in section: the breaker groove behind the edge with a chip curling out of it, and the flank at 7° clearance; made for ISO M.chipcutting edgebreaker grooveclearance 7°ISO groupM
The edge in section; its ISO groups. Not to scale.

What Mitsubishi prints

Insert
Positive
Made for
ISO M (stainless steel)
Cutting area
finishing

Source: Mitsubishi Materials — General Catalog C010A, turning inserts: chip breaker classification (pp. A046–A070) (archived Nov 15, 2026)

FM equivalents

Other makers’ chipbreakers for positive inserts that their own catalogs make for at least one of the same main ISO groups and cutting areas. Equivalent means the same job, not the same shape: check the feed window for your cut.

Other makers’ chipbreakers for the same job
MakerChipbreakerIn commonFeedWhat its maker saysSource
KennametalFPISO M; finishing0.06–0.25 mm/revFinishing steel, stainless, cast iron and high-temperature alloys.

One source: Kennametal, its own catalog

KennametalLFISO M; finishingnot printedFinishing: steel, stainless, cast iron (MT-LF); non-ferrous and high-temperature alloys (GT-LF, precision ground).

One source: Kennametal, its own catalog

KennametalUFISO M; finishing0.05–0.25 mm/revFine finishing of steel, stainless and cast iron.

One source: Kennametal, its own catalog

SandvikMFISO M; finishingnot printedFirst choice for finishing stainless (CoroTurn 107).

One source: Sandvik Coromant, its own catalog

Why FM for austenitic stainless (304, 316)

FM for austenitic stainless (304, 316): Mitsubishi’s finishing geometry for ISO M.

The reasoning, step by step
  1. The situation

    Austenitic stainless work-hardens as it is cut, conducts heat poorly and sticks to the edge. The hardened skin and chips wear a notch in the edge at the depth-of-cut line.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  2. What that means

    A work-hardening alloy needs a sharp, positive edge, and a feed and depth that cut under the layer the last pass hardened. An edge that rubs hardens the next layer.

    Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]

  3. So

    Mitsubishi makes FM (positive) for M in finishing. First recommendation for finishing stainless.

    One source: Mitsubishi Materials, the maker of the chipbreaker , sources [4]

  1. Sandvik Coromant — Workpiece materials: ISO M stainless
  2. Mitsubishi Materials — Machining course: ISO group M, stainless steel
  3. NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
  4. Mitsubishi Materials — General Catalog C010A, turning inserts: chip breaker classification (pp. A046–A070) (archived Nov 15, 2026)

What the cross-reference says

Mitsubishi’s chipbreaker comparison table, a compilation, lists FM for ISO M, finishing. Mitsubishi Materials’ own catalog is the authority for its geometry.

It agrees with Mitsubishi Materials’ catalog.

Source: Mitsubishi Materials USA — Insert Chip Breaker Comparison Table (archived Jul 14, 2024)