Mitsubishi · chipbreaker for negative inserts
GH chipbreaker
Alternative for rough cutting of steel and cast iron; interrupted cuts and scale.
One source: Mitsubishi Materials, its own catalog
What Mitsubishi prints
- Insert
- Negative
- Made for
- ISO P (steel), K (cast iron)
- Cutting area
- roughing
Source: Mitsubishi Materials — General Catalog C010A, turning inserts: chip breaker classification (pp. A046–A070) (archived Nov 15, 2026)
GH equivalents
Other makers’ chipbreakers for negative inserts that their own catalogs make for at least one of the same main ISO groups and cutting areas. Equivalent means the same job, not the same shape: check the feed window for your cut.
| Maker | Chipbreaker | In common | Feed | What its maker says | Source |
|---|---|---|---|---|---|
| Kennametal | RP | ISO P, K; roughing | not printed | Roughing stainless (MG-RP, double-sided); heavy roughing of steel, stainless and cast iron (MM-RP, single-sided). | One source: Kennametal, its own catalog |
| Seco | M5 | ISO P, K; roughing | 0.3–0.7 mm/rev | Roughing with double-sided inserts at high feed in steel, stainless and cast iron. | One source: Seco Tools, its own catalog |
| Seco | RR6 | ISO P; roughing | 0.3–1 mm/rev | Very easy-cutting single-sided roughing of stainless and steel. | One source: Seco Tools, its own catalog |
Why GH for steel
GH for steel: Mitsubishi’s roughing geometry for ISO P.
The reasoning, step by step
The situation
Steel makes chips that are fairly easy to control. The edge’s main enemy is heat, and the harder or higher in carbon the steel, the hotter the edge runs.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
So
Mitsubishi makes GH (negative) for P, K in roughing. Alternative for rough cutting of steel and cast iron; interrupted cuts and scale.
One source: Mitsubishi Materials, the maker of the chipbreaker , sources [3]
What the cross-reference says
Mitsubishi’s chipbreaker comparison table, a compilation, lists GH for ISO P, M, roughing, heavy roughing. Mitsubishi Materials’ own catalog is the authority for its geometry.
- The cross-reference lists it for M; Mitsubishi Materials lists P, K.
- The cross-reference lists it for heavy roughing; Mitsubishi Materials gives roughing.
Source: Mitsubishi Materials USA — Insert Chip Breaker Comparison Table (archived Jul 14, 2024)