Mitsubishi · chipbreaker for negative inserts
HL chipbreaker
First recommendation for heavy cutting of stainless; alternative for steel.
One source: Mitsubishi Materials, its own catalog
What Mitsubishi prints
- Insert
- Negative
- Made for
- ISO M (stainless steel)
- Alternative for
- ISO P (steel)
- Cutting area
- heavy roughing
Source: Mitsubishi Materials — General Catalog C010A, turning inserts: chip breaker classification (pp. A046–A070) (archived Nov 15, 2026)
HL equivalents
Other makers’ chipbreakers for negative inserts that their own catalogs make for at least one of the same main ISO groups and cutting areas. Equivalent means the same job, not the same shape: check the feed window for your cut.
| Maker | Chipbreaker | In common | Feed | What its maker says | Source |
|---|---|---|---|---|---|
| Kennametal | RP | ISO M; heavy roughing | not printed | Roughing stainless (MG-RP, double-sided); heavy roughing of steel, stainless and cast iron (MM-RP, single-sided). | One source: Kennametal, its own catalog |
| Seco | M5 | ISO M; heavy roughing | 0.3–0.7 mm/rev | Roughing with double-sided inserts at high feed in steel, stainless and cast iron. | One source: Seco Tools, its own catalog |
| Seco | RR6 | ISO M; heavy roughing | 0.3–1 mm/rev | Very easy-cutting single-sided roughing of stainless and steel. | One source: Seco Tools, its own catalog |
Why HL for austenitic stainless (304, 316)
HL for austenitic stainless (304, 316): Mitsubishi’s heavy roughing geometry for ISO M.
The reasoning, step by step
The situation
Austenitic stainless work-hardens as it is cut, conducts heat poorly and sticks to the edge. The hardened skin and chips wear a notch in the edge at the depth-of-cut line.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
What that means
A work-hardening alloy needs a sharp, positive edge, and a feed and depth that cut under the layer the last pass hardened. An edge that rubs hardens the next layer.
Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]
So
Mitsubishi makes HL (negative) for M (an alternative for P) in heavy roughing. First recommendation for heavy cutting of stainless; alternative for steel.
One source: Mitsubishi Materials, the maker of the chipbreaker , sources [4]
- Sandvik Coromant — Workpiece materials: ISO M stainless
- Mitsubishi Materials — Machining course: ISO group M, stainless steel
- NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
- Mitsubishi Materials — General Catalog C010A, turning inserts: chip breaker classification (pp. A046–A070) (archived Nov 15, 2026)
What the cross-reference says
Mitsubishi’s chipbreaker comparison table, a compilation, lists HL for ISO P, M, heavy roughing. Mitsubishi Materials’ own catalog is the authority for its geometry.
It agrees with Mitsubishi Materials’ catalog.
Source: Mitsubishi Materials USA — Insert Chip Breaker Comparison Table (archived Jul 14, 2024)