Mitsubishi · chipbreaker for negative inserts
HZ chipbreaker
Alternative for heavy cutting of carbon and alloy steel.
One source: Mitsubishi Materials, its own catalog
What Mitsubishi prints
- Insert
- Negative
- Made for
- ISO P (steel)
- Cutting area
- heavy roughing
Source: Mitsubishi Materials — General Catalog C010A, turning inserts: chip breaker classification (pp. A046–A070) (archived Nov 15, 2026)
HZ equivalents
Other makers’ chipbreakers for negative inserts that their own catalogs make for at least one of the same main ISO groups and cutting areas. Equivalent means the same job, not the same shape: check the feed window for your cut.
| Maker | Chipbreaker | In common | Feed | What its maker says | Source |
|---|---|---|---|---|---|
| Kennametal | RP | ISO P; heavy roughing | not printed | Roughing stainless (MG-RP, double-sided); heavy roughing of steel, stainless and cast iron (MM-RP, single-sided). | One source: Kennametal, its own catalog |
| Seco | M5 | ISO P; heavy roughing | 0.3–0.7 mm/rev | Roughing with double-sided inserts at high feed in steel, stainless and cast iron. | One source: Seco Tools, its own catalog |
| Seco | RR6 | ISO P; heavy roughing | 0.3–1 mm/rev | Very easy-cutting single-sided roughing of stainless and steel. | One source: Seco Tools, its own catalog |
Why HZ for steel
HZ for steel: Mitsubishi’s heavy roughing geometry for ISO P.
The reasoning, step by step
The situation
Steel makes chips that are fairly easy to control. The edge’s main enemy is heat, and the harder or higher in carbon the steel, the hotter the edge runs.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
So
Mitsubishi makes HZ (negative) for P in heavy roughing. Alternative for heavy cutting of carbon and alloy steel.
One source: Mitsubishi Materials, the maker of the chipbreaker , sources [3]
What the cross-reference says
Mitsubishi’s chipbreaker comparison table, a compilation, lists HZ for ISO P, M, heavy roughing. Mitsubishi Materials’ own catalog is the authority for its geometry.
- The cross-reference lists it for M; Mitsubishi Materials lists P.
Source: Mitsubishi Materials USA — Insert Chip Breaker Comparison Table (archived Jul 14, 2024)