Mitsubishi · chipbreaker for negative inserts
LM chipbreaker
First recommendation for light cutting of stainless; high rake controls burrs.
One source: Mitsubishi Materials, its own catalog
What Mitsubishi prints
- Insert
- Negative
- Made for
- ISO M (stainless steel)
- Cutting area
- light cuts
Source: Mitsubishi Materials — General Catalog C010A, turning inserts: chip breaker classification (pp. A046–A070) (archived Nov 15, 2026)
Mitsubishi’s first choice
- For stainless steel under 200 HB (e.g. 304, 316), finishing: LM, with MC7015 (stable), MC7025 (general), MP7035 (unstable).
One source: Mitsubishi Materials, its own catalog
Open the insert pickerLM equivalents
Other makers’ chipbreakers for negative inserts that their own catalogs make for at least one of the same main ISO groups and cutting areas. Equivalent means the same job, not the same shape: check the feed window for your cut.
| Maker | Chipbreaker | In common | Feed | What its maker says | Source |
|---|---|---|---|---|---|
| Seco | MF1 | ISO M; light cuts | 0.08–0.3 mm/rev | Semi-finishing and finishing of stainless, superalloys and titanium. | One source: Seco Tools, its own catalog |
| Seco | MF5 | ISO M; light cuts | 0.2–0.8 mm/rev | Medium finishing of steel and stainless at high feeds. | One source: Seco Tools, its own catalog |
Why LM for austenitic stainless (304, 316)
LM for austenitic stainless (304, 316): Mitsubishi’s light cuts geometry for ISO M.
The reasoning, step by step
The situation
Austenitic stainless work-hardens as it is cut, conducts heat poorly and sticks to the edge. The hardened skin and chips wear a notch in the edge at the depth-of-cut line.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
What that means
A work-hardening alloy needs a sharp, positive edge, and a feed and depth that cut under the layer the last pass hardened. An edge that rubs hardens the next layer.
Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]
So
Mitsubishi makes LM (negative) for M in light cuts. First recommendation for light cutting of stainless; high rake controls burrs.
One source: Mitsubishi Materials, the maker of the chipbreaker , sources [4]
- Sandvik Coromant — Workpiece materials: ISO M stainless
- Mitsubishi Materials — Machining course: ISO group M, stainless steel
- NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
- Mitsubishi Materials — General Catalog C010A, turning inserts: chip breaker classification (pp. A046–A070) (archived Nov 15, 2026)
What the cross-reference says
Mitsubishi’s chipbreaker comparison table, a compilation, lists LM for ISO M, finishing. Mitsubishi Materials’ own catalog is the authority for its geometry.
- The cross-reference lists it for finishing; Mitsubishi Materials gives light cuts.
Source: Mitsubishi Materials USA — Insert Chip Breaker Comparison Table (archived Jul 14, 2024)